In the industrial sector, productive and effective treatment of toxic dye-based color pollutants is a key issue. Lanthanum and neodymium substituted cobalt–strontium (Co–Sr) spinel ferrite (Co0.5Sr0.5RExFe2-xO4, x = 0.00 and 0.06) catalysts were synthesized and used to degrade Congo red and rhodamine B dyes from an aqueous solution mixture in this study. For this specific purpose, RE3+ ions substituted Co–Sr spinel ferrite nanoparticles with photocatalytic degradation ability were prepared through sol–gel method. The degradation of CR and RhB in recently synthesized nanoferrites was also examined. SEM and XRD were used to characterize the prepared samples. The optical band gap values of synthesized spinel ferrites were examined with the help of Tauc plots by using UV-visible absorption. It was determined that the energy bandgap ranged from 2.91 to 2.52 eV. For Co0.5Sr0.5Fe2O4, Co0.5Sr0.5La0.06Fe1.94O4, and Co0.5Sr0.5Nd0.06Fe1.94O4 nanoferrites, the rates of CR and RhB dye degradation were 73–90% and 45–85%, respectively, at pH 5–7. The kinetics models successfully described the degradation reaction as pseudo-first-order kinetics. It was, therefore, concluded that the prepared samples can be used as effective photocatalysts in order to eliminate hazardous pollutants present in wastewater.
These days, water contamination poses a severe threat to the ecosystem and demands immediate care. This study examined the need to reduce water pollution using clean, renewable energy (solar light irradiations) for the degradation of Congo red by Silver-indium and antimony selenide with chemical composition AgInSbSe3. The sample was fabricated through a hydrothermal technique. The synthesized sample was characterized through X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), Scanning electron microscopy (SEM) and Ultraviolet-Visible spectroscopy. The X-ray diffraction confirms crystalline structure of the synthesized sample. The SEM analysis reveals irregular grains and exhibits a very small inter-particle distance. SEM provides the morphology of the synthesized sample, the grain size of the synthesized sample was 0.58 μm. FTIR results revealed specific absorption bands in the range of 400–4000 cm−1; optical properties are studied through UV-Vis-spectroscopy. The synthesized sample has 1.97 eV bandgap which is suitable for degradation of organic pollutants. The photocatalytic activity of the material is checked by degrading the Congo red dye under direct sunlight irradiation and for the 75 min illumination 77.8% degradation efficiency is attained.