6 October 2017 in IEEE Transactions on Nuclear Science
The degradation induced by ultra-high total ionizing dose in 65 nm MOS transistors is strongly gate-length dependent. The current drive decreases during irradiation, and the threshold voltage often shifts significantly during irradiation and/or high-temperature annealing, depending on transistor polarity, applied field, and irradiation/annealing temperature. Ionization in the spacer oxide and overlying silicon nitride layers above the LDD extensions leads to charge buildup as well as the ionization and/or release of hydrogen. Charge trapped in the spacer oxide or at its interface modifies the parasitic series resistance, reducing the drive current. The released hydrogen transports as H+ with an activation energy of ~ 0.92 eV. If the direction of the electric field is suitable, the H+ can reach the gate oxide interface and de-passivate Si-H bonds, leading to threshold voltage shifts. Newly created interface traps are most prominent near the source or drain. The resulting transistor responses and defect-energy distributions often vary strongly in space and energy as a result, as demonstrated through current-voltage, chargepumping, and low-frequency noise measurements.
1 October 2018 in IEEE Transactions on Nuclear Science
Significant threshold voltage Vth shifts are observed during 10-keV X-ray irradiation of AlGaN/GaN HEMTs. Shifts are much smaller for lower-dose-rate Cs-137 irradiation than for higher-dose-rate X-ray irradiation. This occurs because hydrogen transport and interactions with defects and impurities in these crystalline wide band-gap semiconductor materials differ fun-damentally from those in amorphous SiO2. The electric field is also higher in GaN-based HEMTs than in bipolar base oxides. The absence of ELDRS in these devices simplifies testing of GaN-based HEMTs for space applications. No significant X-ray induced Vth shifts are observed for development stage InAlN/GaN HEMTs.
19 December 2019 in IEEE Transactions on Nuclear Science
Total-ionizing-dose effects and low-frequency noise are evaluated in 30 nm gate-length bulk and SOI FinFETs for devices with fin widths of 10 nm to 40 nm. Minimal threshold voltage shifts are observed at 2 Mrad(SiO2), but large increases in low-frequency noise are found, and significant changes in defect-energy distributions are inferred. Radiation-induced leakage current is enhanced for narrow- and short-channel bulk Fin-FETs. Short-channel SOI FinFETs show enhanced degradation compared with longer-channel devices. Narrow- and short-channel SOI devices exhibit high radiation tolerance. Significant random telegraph noise is observed in smaller devices due to prominent individual defects.
17 November 2017 in IEEE Transactions on Nuclear Science
The radiation hardness of AlGaN/GaN high-electron-mobility transistors (HEMTs) is found to improve with increasing GaN channel thickness. Epitaxial MgCaO shows promise as a radiation-tolerant gate dielectric, with only small shifts in operating parameters of metal-oxide-semiconductor HEMTs observed at doses up to 1 Mrad(SiO2). Bias-induced electron trapping and radiation-induced-hole trapping can occur in the MgCaO, depending on the applied bias during stress and/or irradiation. AC transconductance measurements are used to help understand charge trapping in these devices.
3 January 2019 in IEEE Transactions on Nuclear Science
10 October 2017 in IEEE Transactions on Nuclear Science
We have performed a detailed evaluation of radia-tion-induced charge trapping and low-frequency noise for back-gated graphene transistors fabricated on a thermal SiO2 layer, with Al2O3 or h-BN passivation over-layers. Irradiation with positive or 0 V back-gate bias leads to negative shifts of the charge neutral point (CNP) of the graphene transistors; irradia-tion under negative back-gate bias leads to positive CNP shifts. The low-frequency noise increases with irradiation and decreases with 400 K post-irradiation annealing. The temperature de-pendence of the noise is described well by the Dutta-Horn model of low-frequency noise. Peaks in effective defect-energy distribu-tions of irradiated devices at ~ 0.4 eV and ~ 0.7 eV are identified via measurements of the temperature dependence of the low-frequency noise. The noise of as-processed devices stored in room ambient also decreases with baking, but does not show the clear peaks observed after irradiation. Density functional theory calculations suggest that OH− and H+ at or near the gra-phene/dielectric interfaces likely play key roles in both the irra-diation and baking response. Low-frequency noise and CNP voltage shifts during switched-bias post-irradiation annealing at room temperature also suggest significant roles for O vacancies in the near interfacial SiO2 and/or passivation layers.