29 April 2020 in IEEE Electron Device Letters
This letter reports the polymer passivation of field plated lateral $\beta $ -Ga 2 O 3 MOSFETs with significant improvement in the breakdown voltages as compared to non-passivated devices. We show consistent results of higher breakdown voltages in passivated devices as compared to non-passivated devices for MOSFETs with $\text{L}_{\textit {gd}}$ ranging from $30~\mu \text{m}$ to $70~\mu \text{m}$ and across two process runs. We obtain a record high breakdown voltage of 6.72 kV for a MOSFET with $\text{L}_{\textit {gd}}= {40}\mu \text{m}$ giving an average field strength of 1.69 MVcm −1 . The peak drain current is $\sim ~3$ mA/mm for $\text{L}_{g}= {2}\mu \text{m}$ device with a gate source separation of $3~\mu \text{m}$ . The on-resistance for the device is, $\text{R}_{\textit {on}}= {13}\,\,\text{k}\Omega ^{.}$ mm, giving a power device Figure of Merit of 7.73 kWcm −2 . The $\text{R}_{\textit {on}}$ is high due to plasma induced damage of channel and access regions. The $\text{R}_{\textit {on}}$ and on-current density remain unchanged after passivation. The breakdown increases with $\text{L}_{\textit {gd}}$ up to 70 $\mu \text{m}$ , giving a maximum breakdown voltage of 8.03 kV.
1 May 2023 in Applied Physics Letters
This Letter reports a high performance β-Ga2O3 thin channel MOSFET with T gate and degenerately doped (n++) source/drain contacts regrown by metal organic chemical vapor deposition. Highly scaled T-gate with a gate length of 160–200 nm was fabricated to achieve enhanced RF performance and passivated with 200 nm silicon nitride. Peak drain current (ID,MAX) of 285 mA/mm and peak transconductance (gm) of 52 mS/mm were measured at 10 V drain bias with 23.5 Ω mm on resistance (RON). Metal/n++ contact resistance of 0.078 Ω mm was extracted from transfer length measurements. RON is possibly dominated by interface resistance between channel and highly doped n++ regrown layer. A gate-to-drain breakdown voltage of 192 V is measured for LGD = 355 nm resulting in average breakdown field (EAVG) of 5.4 MV/cm. This EAVG is the highest reported among all sub-micron gate length lateral FETs. Current gain cut off frequency (fT) of 11 GHz and record power gain cut off frequency (fMAX) of approximately 48 GHz were extracted from small signal measurements. fT is limited by DC-RF dispersion due to interface traps which needs further investigation. The fT·VBR product is 2.112 THz V for 192 V breakdown voltage. Device surpasses the switching figure of merit of Silicon and competitive with mature wide bandgap devices.
1 November 2022 in IEEE Electron Device Letters
This letter reports vacuum annealing of lateral field-plated β-Ga 2 O 3 MOSFETs with significant current recovery and improvement in the on-state resistance, R on , after Reactive Ion Etching (RIE) induced damage. We fabricate and characterize MOSFETs based on Molecular Beam Epitaxy (MBE) and Metal-Organic Chemical Vapor Deposition (MOCVD) grown β-Ga 2 O 3 wafers to better understand the effects of vacuum annealing. We see a clear trend of vacuum annealed devices showing no reduction in breakdown voltages, V br , as compared to polymer passivated MOSFETs. This trend holds for identical gate-drain separation, L gd , varying from 20 μm to 60 μm. Devices show up to 10 times reduction in R on as compared to previously reported R on for SU-8 passivated devices. For MBE sample, V br of 7.16 kV for a L gd = 40 μm device, with an average field strength of 1.79 MVcm -1 and peak drain current density of 40 mA/mm, is reported. R on is 897 Ω∙mm, giving Baliga’s Figure of Merit (BFOM) as 5.71 MWcm -2 . For a L gd = 60 μm device, we report record high breakdown of 8.56 kV with BFoM of 4.9 MWcm -2 . For MOCVD grown sample, a L gd = 60 μm device has V br of 6.11 kV, R on of 1.98 kΩ∙mm and corresponding BFoM of 1.88 MWcm -2 . Transfer Length Method (TLM) analysis indicates incomplete post etch current recovery after vacuum annealing.
1 June 2023 in APL Materials
Atomic scale details of the formation of point defects and their evolution to phase transformation in silicon (Si) implanted β-Ga2O3 were studied using high resolution scanning transmission electron microscopy (STEM). The effect of Si implantation and the formation of defects was studied as a function of the dose of implanted atoms, and the detailed mechanism of lattice recovery was observed using both in situ and ex situ annealing of the implanted β-Ga2O3. The implantation created nanoscale dark spots in STEM images, which we identified as local γ-Ga2O3 inclusions generated by the relaxation of lattice due to ⟨010⟩ screw dislocations created by the implantation. The number and size of γ-Ga2O3 regions increased as the Si dose increased, and eventually the γ-Ga2O3 crystal phase (with stacking defects) took over the entire implanted volume when the peak Si concentration was over ∼1020 cm−3. Annealing above 1100 °C disintegrates the local γ-Ga2O3 phase and returns the structure to defect-free, single crystal β phase, likely indicating that point defects (such as Si interstitials and cation vacancies) are spatially redistributed by the annealing. However, when the structure is completely transformed to γ-Ga2O3 by the implantation, post-annealing leaves a high concentration of dislocations within the β phase, which relates to the inhomogeneous distribution of Si atoms detected by secondary ion mass spectrometry.