Chair for Electrochemical Energy Conversion and Storage Systems, Institute for Power Electronics and Electrical Drives (ISEA), RWTH Aachen University, Aachen 52074, Germany
Auto-generated profile, based on publicly available information
Sebastian Klick
Chair for Electrochemical Energy Conversion and Storage Systems, Institute for Power Electronics and Electrical Drives (ISEA), RWTH Aachen University, Aachen 52074, Germany
Sodium‐ion batteries offer a promising alternative to lithium‐ion batteries by addressing ecological and economic challenges. However, to assess the applicability of these cells for different sectors, understanding aging behavior, including degradation modes, is crucial. This work presents a comprehensive aging analysis of 67 commercial sodium‐ion batteries under various temperatures, C‐rates, and depths of discharge. We analyzed the initial cell‐to‐cell variance and the aging trajectories regarding capacity fade and resistance increase. We demonstrated that the cycling rate does not significantly influence the aging trajectories, whereas smaller depths of discharge significantly reduce degradation. The degradation gradients for 25 °C and 40 °C were similar; for −10 °C, we observed rapid capacity fading that can be attributed to irreversible sodium plating. Furthermore, we identified the degradation modes for four different aging categories. Since some aging tests stopped due to gas‐induced current interrupt device triggering at low current rates and states of charge, we proposed two hypotheses for the gassing under specific conditions, suggesting inadequate gas consumption in cathode‐electrolyte side reactions or solid electrolyte interphase instability as potential causes. Overall, this work provides a valuable in‐depth analysis of the aging behavior of a commercial sodium‐ion battery as a function of temperature, C‐rate, and depth of discharge, with data made available for further research.
Calendaric lifetime testing of lithium‐ion cells is time‐consuming and resource‐intensive. As Dubarry et al.[1] state, testing is often limited to a few aging conditions. This paper presents the results of a long‐term aging study on lithium‐ion cells with a nickel‐rich NCA cathode and a graphite‐silicon anode. 69 cells were stored at 5 different voltages and under 4 different temperatures for 5 years. Regular reference performance tests (RPT) provide insights for State of Health (SoH) calculation and further analysis through differential voltage analysis. The results are verified against post‐mortem analyses. The long aging period enables accurate determination of aging rates. Our results demonstrate that the storage voltage level strongly influences the degradation rate, with temperature playing a minor role. The identified aging effects include loss of active material on the cathode side and loss of lithium inventory. Initial degradation follows a ‐trajectory but is caused by overhang effects. The long‐term aging is rather linear.
Lithium‐ion cells with graphite anodes and nickel–manganese–cobalt oxide (NMC622) cathodes are filled with three different amounts of electrolyte. During formation, incremental capacity analysis indicates small differences in the formation processes between cells with insufficient electrolytes to fill all pores and those with an electrolyte volume above the total pore volume of the cell. Complimentary analysis of the gases developed during formation shows that the composition of these cells differs from the cells with a sufficient electrolyte. The aging of cells under high temperature (60 °C) and high constant voltage of 4.2 V is studied. During aging, cells with higher amounts of electrolyte degrade substantially slower. Based on data available from electrical tests, a theory explaining the volume‐dependent rise of resistance and capacity decay is proposed.
1 July 2025 in Journal of the Electrochemical Society
The effect of the electrolyte on lithium-ion battery degradation is a subject of current research. In this publication we present the investigation of a total of 16 cells divided into 4 groups based on the anode material (graphite and SiOx-graphite composite) and the electrolyte volume (3.5 ml as recommended by the manufacturer and 2.8 ml). Cells were aged with a low-current cyclic ageing regime at elevated temperatures of 45 °C. Cells with SiOx-containing anodes suffer substantial loss of active material during the initial cycles regardless of electrolyte volume, whereas degradation of cells with graphite-anodes depend heavily on the electrolyte volume. Cells with 2.8 ml exhibit a knee-point after about 100 cylces, whereas those with 3.5 ml exhibit a linear capacity fade until well over 300 cycles. The knee-point coincides with substantial loss of lithium, and loss of active anode material.
The purpose of this study was to investigate the calendar aging of lithium-ion batteries by using both open circuit and floating current measurements. Existing degradation studies usually focus on commercial cells. The initial electrolyte composition and formation protocol for these cells is often unknown. This study investigates the role of electrolyte additives, specifically, vinylene carbonate (VC) and fluoroethylene carbonate (FEC), in the aging process of lithium-ion batteries. The results showed that self-discharge plays a significant role in determining the severity of aging for cells without additives. Interestingly, the aging was less severe for the cells without additives as they deviated more from their original storage state of charge. It was also observed that the addition of VC and FEC had an effect on the formation and stability of the solid electrolyte interphase (SEI) layer on the surface of the carbonaceous anode. By gaining a better understanding of the aging processes and the effects of different electrolyte additives, we can improve the safety and durability of lithium-ion batteries, which is critical for their widespread adoption in various applications.