The coarse-grained heat-affected zone specimens of X80 pipeline steel were produced by welding thermal simulation under different heat inputs of 10, 30, and 55 kJ/cm to study the effects of heat input on microstructure evolution and corrosion characterization. The corrosion resistance of coarse-grained heat-affected zones was poorer than that of base metal due to less homogenous in the former. For 10 kJ/cm coarse-grained heat-affected zone, the corrosion resistance was poorer than the others due to the more adsorption hydrogen around the needle-like martensite/austenite constituents and greater galvanic driving force between the needle-like martensite/austenite constituents and ferrite. In carbonate/bicarbonate solution, better corrosion resistance for coarse-grained heat-affected zones was obtained when the heat input is 30 kJ/cm, which can be attributed to the severe coarse martensite/austenite constituents for 55 kJ/cm coarse-grained heat-affected zone. In the H2S environment, the better corrosion resistance for coarse-grained heat-affected zone was obtained when the heat input is 55 kJ/cm, which can be attributed to the protective effect of corrosion products. In addition, the high content of M/A constituents for 30 kJ/cm CGHAZ was good for hydrogen adsorption, which was adverse to the corrosion resistance in acid environments.
The corrosion behavior of copper-nickel alloy/carbon steel couple, subjected to a sulfide-containing simulated seawater environment beneath an artificially defective epoxy coating, was systematically investigated using a combination of wire beam electrode (WBE), electrochemical impedance spectroscopy, and microscopic characterization techniques. The results indicate that the anodic reaction at the artificial defect during the early stages of immersion is the most intense. A broad spectrum of cathodic currents is observed at the coating/metal interface. As immersion time progresses, the artificial defects are progressively protected by the corrosion product iron sulfide, resulting in a gradual attenuation of the anodic reaction. A significant disparity in the degree of cathodic delamination exists between coupled copper-nickel alloy and carbon steel beneath the epoxy coating. It can be attributed to their different electrochemical activities and the specific location of the artificial defect on the WBE. Throughout the immersion process, the copper-nickel alloy is less eroded. This phenomenon can be attributed to the protective effect of copper oxide and basic copper chloride films and the microgalvanic effect. In the region of carbon steel, multiple anodes are positioned at the immersed end. In addition, the reasons why individual carbon steel electrodes exhibit polarity reversal vary at different immersion stage.