1 May 2011 in Journal of Materials Processing Technology
1 August 2009 in International Journal of Material Forming
15 July 2007 in Key Engineering Materials
Hemming is the last or one of the latest stage operations for the stamped parts. For this reason it has a critical importance on the performance and perceived quality of assembled vehicles. It is used to attach two sheet metal parts together or to improve appearance creating a smooth edge rather than a razor edge with burrs. However, designing the hemmed union is not always easy and is deeply influenced by the mechanical properties of the material of the bended part. Main problems for the automotive industry arise when bending aluminum alloys. Aluminum sheet is more difficult to hem due to its susceptibility to strain localization during the hemming process. This phenomenon produces cracking on the hemmed edge [1]. In order to avoid this problem and due to the limitations of conventional flanging and hemming technologies, the flange radii must be increased and a rope hem used (instead of the flat hem used with steels) when working with aluminum alloys. These changes on the design of the hem union give as a result a lower quality final product [2]. Dies and tools used for the hemming process are designed based on experience and on lengthy and costly die tryouts. Continuing with the development of new applications for the Electromagnetic Forming (EMF) technology, LABEIN-Tecnalia and Professor Glenn Daehn’s group from The Ohio State University carried out some first straight flat hemming experiments using the AA 6016 T4 aluminum alloy. The results obtained from these first trials are presented in this paper giving a first sight of the possibilities, advantages and disadvantages of using the Electromagnetic Forming technology for the hemming of aluminum sheet panels. Using a non-clouped FEM simulation method, the experimental results are compared to the ones obtained with the simulations. The future working line in developing this new application for the Electromagnetic Forming technology will be based on the results obtained by this study.
28 September 2019 in SN Applied Sciences
The paper shows the investigation results of correlating electric discharge and pressure field parameters aimed to improvements in the electrohydraulic impact forming (EHF) technology at industrial application. The experimental research was performed by using a conical discharge chamber equipped with a set of two electrodes in semi-industrial EHF installation. Pressure fields along round flat area were measured by applying the multi-point membrane pressure gauge methodology. The conditions of the tests include a wide range of spark gaps with four levels of charge voltage and energy. Measurements of discharge voltage and current are performed with voltage divider, Rogovsky coil and electronic oscilloscope. Other electric discharge parameters were calculated from the recorded voltage and current curves. The essence of investigation is to analyse energy parameters for peak pressure of shock wave generated by these discharge energy parameters. Though these dependencies were earlier analysed theoretically and tested in electrohydraulic plants under laboratory conditions, the practical interest in this experimental investigation is to reveal influence of conditions of real semi-industrial EHF press designed for batch production of sheet parts. Conducted experimental investigation has shown that industrial applications of high-voltage non-initiated discharges can significantly deviate from the theoretical and laboratory results. Dependencies of peak pressure from maximum power during the first semi-period of discharge current and slope of power curve appeared to be not so strong. These deviations in peak pressure can reach 20–30%. Among the assumed additional factors influencing energy and pressure parameters are: condition of current-conductive rod of electrode (erosion, rust, radius); condition (wear) of electrode insulator (increase of naked area of current-conductive rod); variations in shape, position and length of discharge channel relative to spark gap; “shadowing” effect of electrodes at some positions of discharge channel relative to electrode;, several discharge channels at small spark gap and other. To reveal effect of these factors the authors plan to carry-out tests with wire-initiated discharges to check the variations in shape, position and length of discharge channel relative to spark gap in the same discharge chamber configuration.
26 December 2018 in Materials Science Forum
In cold forming for automotive lightweight design, advanced high strength steels (AHSS) lead to limited formability, high springback and press forces, low stretch flangeability, multiple operations for complex geometries and large scrap rates. Two sets of AHSS, namely ferritic-martensitic dual-phase (DP) steel and martensitic-bainitic complex-phase (CP) steel with some amounts of retained austenite (RA), were designed for the hot-forming route, which eliminates the above drawbacks and guarantees higher performance in the body-in-white (BIW). Design of four DP and four CP alloys was accomplished using JMatPro6.0 thermodynamic software and available literature. The alloys were manufactured in the laboratory in cold-rolled gauge of ~1.5 mm and subjected to hot-forming cycles including hot deformation (up to 20% strain), using a dilatometer and a Gleeble 3800 machine. The thermal cycles of the DP alloys included an intercritical reheating whereas in-situ austempering or slow continuous cooling followed by supercritical reheating was used for the CP alloys. The results showed that yield strength (YS) of 605MPa & 695MPa, ultimate tensile strength (UTS) of 1097MPa & 1242MPa with a total elongation (TE) of 12.6% & 14.1% can be achieved in the best performing DP alloys with a martensite content of 65% & 60 vol.%. The best CP alloys with austempering achieved YS of 673MPa & 699MPa, UTS of 983MPa & 1026MPa and TE of 9.2% & 13.6% with RA of 4%-12 vol.%. The continuously-cooled alloys achieved even better properties. Higher bendability at 1.0 mm gauge in the critical direction was achieved in the CP alloys (90o&107o) than in the DP alloys (73o&76o).