Sina Soltanmohammad

Sina Soltanmohammad

Auto-generated profile, based on publicly available information

Sina Soltanmohammad

Tower Semiconductor, Newport Beach CA

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
30 December 2019 in IEEE Journal of Photovoltaics
Verified
Journal Article
Closed access
SKShankar Karki
Shankar Karki
JDJulia I. Deitz
Julia I. Deitz
GRGrace Rajan
Grace Rajan
SSSina Soltanmohammad
Sina Soltanmohammad
DPDeewakar Poudel
Deewakar Poudel
Sylvain MarsillacSylvain Marsillac
Sylvain Marsillac
Solar cell degradation can occur through many pathways and at the different stages of the fabrication process, notably because of the water condensation. In the case of Cu(In,Ga)Se 2 (CIGS) solar cells, the impact of water ingress on Mo back contact can be substantial for not only the film itself but also the device performance and reliability. Microstructural modification, change in film morphology, loss in reflectance, and increased resistivity because of the moisture ingress were observed via X-ray diffraction, transmission electron microscopy, spectroscopic ellipsometry, and four-point probe measurements, respectively. Secondary ion mass spectrometry measurements revealed drastic changes in the alkali (Na, K) profiles in both the CIGS and Mo layers, likely because of the modification of their diffusion coefficient through Mo. This, in turn, negatively impacts the solar cell efficiency by decreasing both fill factor and open-circuit voltage. Additional experiments, modifying the substrate and utilizing a NaF postdeposition treatment, highlight the mechanisms of degradation as being due to both a modification of the Mo/CIGS interface and the lack of alkali diffusion after water ingress.

1 November 2019 in Thin Solid Films
Verified
Journal Article
Closed access
GRGrace Rajan
Grace Rajan
BBBenjamin Belfore
Benjamin Belfore
SKShankar Karki
Shankar Karki
DPDeewakar Poudel
Deewakar Poudel
HKHamza Kahoui
Hamza Kahoui
Sylvain MarsillacSylvain Marsillac
Sylvain Marsillac

6 January 2021 in Journal of Energy and Power Technology
Verified
Journal Article
Open access
PDF file
DPDeewakar Poudel
Deewakar Poudel
BBBenjamin Belfore
Benjamin Belfore
SKShankar Karki
Shankar Karki
GRGrace Rajan
Grace Rajan
SSSina Soltanmohammad
Sina Soltanmohammad
Sylvain MarsillacSylvain Marsillac
Sylvain Marsillac
The effect of water ingress on the surface of the buffer layer of a Cu(In, Ga)Se2 (CIGS) solar cell was studied. Such degradation can occur either during the fabrication process, if it involves a chemical bath as is often the case for CdS, or while the modules are in the field and encapsulants degrade. To simulate the impact of this moisture ingress, devices with a structure sodalime glass/Mo/CIGS/CdS were immersed in deionized water. The thin films were then analyzed both pre and post water soaking. Dynamic secondary ion mass spectroscopy (SIMS) was performed on completed devices to analyze impurity diffusion (predominantly sodium and potassium) and to assess potential degradation mechanisms. The results were compared to device measurements, which indicate a degradation of all device parameters due to an increase in the total and peak trap densities, as shown by simulation. This is potentially due to a modification of the sodium profile in the bulk CIGS, with a decrease content after water soaking or because the oxygen profile increased in the bulk CIGS after water soaking.

25 February 2019 in IEEE Journal of Photovoltaics
Verified
Journal Article
Closed access
SSSina Soltanmohammad
Sina Soltanmohammad
HTHo Ming Tong
Ho Ming Tong
TATimothy J. Anderson
Timothy J. Anderson
WSWilliam N. Shafarman
William N. Shafarman
The addition of Ag to Cu-Ga-In precursors for synthesizing (Ag,Cu)(In,Ga)Se $_2$ (ACIGS) thin films has shown benefits including improved adhesion, greater process tolerance, and potential for improved device performance. In this study, reaction pathways to form Cu(In,Ga)Se $_2$ (CIGS) and ACIGS were studied by time-progressive reactions at 450 °C in a 5% Ar/H $_2$ Se atmosphere followed by ex situ characterization. Results indicated that the addition of 25% Ag/(Ag+Cu) to the CIGS film reduces the reaction time by 50%. X-ray diffraction (XRD) analysis of CIGS films showed that the CuInSe $_2$ phase initially formed after 3.5 min. The slow reaction of the stable γ-Cu $_9$ (In,Ga) $_4$ phase, however, required more than 20 min to complete. Importantly, the addition of Ag to the CIGS film accelerated the reaction. Energy-dispersive X-ray spectroscopy shows that Ga/(Ga+In) grading occurs in the first 10 min of the reaction. XRD analysis showed that the chalcopyrite phase fully forms after 10 min and no significant changes were observed in samples selenized from 10–45 min. Reaction pathways of Ag-alloyed films were further characterized using in situ high temperature XRD analysis. The onset temperature of Se reaction was detected at 230 °C and a AgIn $_2$ phase transformation to (Ag,Cu)In $_2$ occurred during the early stage of the reaction.

1 July 2017 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
SSSina Soltanmohammad
Sina Soltanmohammad
BMBrian McCandless
Brian McCandless
WSWilliam N. Shafarman
William N. Shafarman

14 June 2020
Verified
Conference Paper
Closed access
HTHo Ming Tong
Ho Ming Tong
SSSina Soltanmohammad
Sina Soltanmohammad
WSWilliam N. Shafarman
William N. Shafarman
TATimothy J. Anderson
Timothy J. Anderson
The substitution of Ag for Cu in Cu(Ga, In)Se 2 has been shown to optimize the bandgap of the chalcopyrite while decreasing defect density and formation temperature. The synthesis of chalcopyrite via selenization of metal precursor films with a complete substitution of Ag for Cu was studied both in-situ during selenization using high temperature x-ray diffraction and ex-situ using electron microcopy. AgInSe 2 formation at low temperatures was limited by the availability of Ag in the liquid phase resulting in the formation of Ag-deficient Ag-In-Se phases. Ga alloying into AgInSe 2 at high temperature was limited by the stability of (Ga, In) 2 Se 3 .