This letter demonstrates vertical GaN junction barrier Schottky (JBS) rectifiers fabricated with novel ion implantation techniques. We used two different methods to form the lateral p-n grids below the Schottky contact: 1) Mg implantation into n-GaN to form p-wells and 2) Si implantation into p-GaN to form n-wells. Specific differential ON-resistances ( ${R}_{ \mathrm{\scriptscriptstyle ON}}$ ) of 1.5–2.5 $\text{m}\Omega ~\cdot $ cm 2 and 7–9 $\text{m}\Omega ~\cdot $ cm 2 were obtained in the Mg-implanted and Si-implanted JBS rectifiers, respectively. A breakdown voltage of 500–600 V was achieved in both devices, with a leakage current at high reverse biases at least 100-fold lower than conventional vertical GaN Schottky barrier diodes. The impact of n-well and p-well widths on the ${R}_{ \mathrm{\scriptscriptstyle ON}}$ and BV was investigated. Fast switching capability was also demonstrated. This letter shows the feasibility of forming patterned p-n junctions by novel ion implantation techniques, to enable high-performance vertical GaN power devices.
Record DC power has been demonstrated in AlGaN/GaN high electron mobility transistors fabricated using a substrate replacement process in which a thick diamond substrate is grown by chemical vapor deposition following removal of the original Si substrate. Crucial to the process is a ~30 nm thick SiN interlayer that has been optimized for thermal resistance. The reductions obtained in self-heating have been quantified by transient thermoreflectance imaging and interpreted using 3D numerical simulation. With a DC power dissipation level of 56 W/mm, the measured average and maximum temperatures in the gate-drain access region were 176 °C, and 205 °C, respectively.
A long‐standing goal of GaN device research has been the development of a reliable, well‐controlled process for p‐GaN formation by ion implantation. Results to date have indicated an activation of 1% or less using high‐temperature rapid thermal annealing (RTA) techniques and coimplantation. Although Mg is a relatively deep acceptor, this is still much less than the theoretically achievable value (8.2% based on the 160 meV acceptor level). A multicycle RTA process is presented that is capable of achieving up to 8% activation of the Mg‐implanted GaN. This approaches the theoretical value, and represents a significant step in GaN device research.
20 October 2020 in IEEE Transactions on Electron Devices
Gallium nitride (GaN) high electron-mobility transistors (HEMTs) offer considerable high-power operation but suffer in reliability due to potentially damaging self-heating. In this study, self-heating in AlGaN/GaN HEMTs on high conductivity substrates is assessed using a high-resolution thermoreflectance (TR) imaging technique, to compare the thermal response between GaN-on-Si, GaN-on-Diamond, and GaN-on-4H-SiC. The TR method accuracy at high-power density is verified using a nonlinear coefficient of TR (CTR) as a function of temperature. The acquired steady-state thermal maps give a thermal resistance of 11.5 mm · K/W for GaN-on-Si (based on peak channel temperature), compared to 2.7 and 3.3 mm · K/W for GaN-on-SiC and GaN-on-diamond substrates, respectively. The tested GaN-on-diamond HEMT exhibits similar heating rates to those seen on a SiC substrate, with a slightly higher peak temperature, which indicates a higher thermal boundary resistance that could offset the benefits of using a higher conductivity substrate and lead to faster thermally enhanced degradation. The analysis reveals the importance using high-resolution imaging to detect hotspots and areas of peak temperature that largely affect failure initiation and device reliability and which may not be otherwise observable.
30 June 2009 in Journal of Vacuum Science & Technology A
GaN films were grown on Si(100) substrate by atomic layer deposition (ALD) using GaCl3 and NH3. Growth conditions were identified for which the growth rate exhibited a plateau at ∼2.0Å∕cycle, consistent with self-limiting adsorption. A relatively wide temperature window (500–750°C) for ALD growth mode was also established for one flow sequence schedule. In this limit, both the (0002) and (101¯1) orientations of GaN were evident, which was attributed to the competition between vertical and lateral growths. Cl incorporation was detected by x-ray photoelectron spectroscopy for samples prepared with long GaCl3 exposure time. It is postulated that gas phase formation of (ClGaNH)n with n=1–3 [Kovács, Inorg. Chem. 41, 3067 (2002)] results in higher Cl content.