Leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) at 20 and 90°C in mineralized water simulating the composition of underground waters on the site
Experiments on leaching of borosilicate glass samples containing 10, 15, and 20 wt % simulated high-level waste (HLW) were performed at 20 and 90°C in hydrogen peroxide solutions. H2O2 was used as a substance simulating products of underground water radiolysis. The leach rates and diffusion coefficients of the glass components were determined. The character and extent of the effect of the varied experimental parameters on the characteristics being determined were evaluated by correlation analysis. The presence of hydrogen peroxide in the contact solution enhances the chemical durability of borosilicate glasses.
Borosilicate glass specimens incorporating 10, 15, and 20 wt % simulated high-level waste (HLW) were leached at 20, 90, and 120°C in deionized water following the procedure accepted in Russia, GOST (State Standard) R 52 126-2003. At 90°C, the altered surface layer is formed already from the first days of leaching. The main interaction in the system occurs at the phase boundary between the altered surface layer and water, rather than at the phase boundary between the glass and water through the porous surface layer as it is commonly believed. The altered surface layer acts as a natural barrier preventing transfer of simulated waste components to the liquid phase. The barrier properties of the altered surface layer are manifested to the greatest extent at 20 wt % content of simulated HLW in the initial glass and leaching temperature of 120°C.
At the Khlopin Radium Institute, during the development of extractive partitioning of the liquid high-level radioactive waste (HLW), a strip solution containing up to 6.0 × 1011 Bq/dm3 (16.3 Ci/dm3) of 137Cs in the form of a nitric acid solution was collected and temporary was stored. To solidify this solution, a batch process using Gubka (sponge) porous inorganic material (PIM) was developed and implemented. Since that time, about 18 dm3 of HLW was solidified into 12 sets of Gubka, reducing the liquid HLW volume by a factor of about 50. Gubka sets were placed into special containers, which after sealing by welding were delivered to the long-time storage of the RosRAO Branch in Sosnovy Bor.