First-principles calculation of D022 Mn3Ge shows a fully spin-polarized ?1 band at the Fermi level, low saturation magnetization MS=180 emu/cm3, high uniaxial magnetic anisotropy Ku=23 Merg/cm3, and low Gilbert damping ?=9?10-4. We also experimentally investigate D022 Mn3+xGe epitaxial films grown on MgO(100) substrates with different compositions x. The films exhibit a coercivity of about 20 kOe, MS of about 130 emu/cm3, and Ku of about 10 Merg/cm3 at x=0.55 (78 at.% Mn). These indicate that D022 Mn3Ge is a good candidate for spin-transfer-torque random access memory.
We prepared D022-Mn3+xGe (−0.67 ≤ x ≤ 0.35) epitaxial thin films on MgO(001) substrates with Cr(001) buffer layers and systematically investigated the dependence of their perpendicular magnetic anisotropy constant, saturation magnetization, coercivity, and tetragonal axial ratio (c/a) on their composition and substrate temperature. Single-phase D022 crystal structures were formed in films with compositions of 0 ≤ x ≤ 0.35, prepared at 400 °C. The D022-Mn3Ge films exhibited perpendicular magnetization with a magnetic squareness close to unity. Performing magnetic torque measurements at an applied field of 140 kOe, we estimated a perpendicular magnetic anisotropy constant of 11.8 ± 0.5 Merg/cm3, the highest and the most reliable value yet reported.
Epitaxial growth and magnetization precessional dynamics for tetragonal MnAlGe films are investigated. The films are grown on MgO (100) with c axis parallel to the film normal and well-ordered layered structures. The film exhibits rectangular hysteresis loop with perpendicular magnetic anisotropy constant of 4.7 Merg/cm3 and saturation magnetization of 250 emu/cm3. Magnetization precession with precession frequency of ∼100 GHz is observed by time-resolved magneto-optical Kerr effect. Further, the Gilbert damping constant is found to be less than ∼0.05, which is much larger than that obtained using the first principles calculations.
We developed a fully epitaxial magnetic tunnel junction on an 8″ silicon wafer by using a mass-production sputtering apparatus and achieved a high magnetoresistance ratio exceeding 240% at room temperature. One of the key factors in this achievement is the use of a B2-type Ni-Al seed layer on the wafer as a (001)-oriented and an atomically smooth template. Another is the insertion of a thin Al layer prior to MgO sputtering as protection from plasma damage, resulting in the formation of a spinel-type single-crystal Mg-Al-O tunnel barrier after in situ annealing. This epitaxial technology for transition metals on large wafers will lead to advanced practical spintronics devices incorporating high-performance single-crystalline materials such as chemical-ordered alloys and tunnel barriers.
We developed a surface smoothing technique for stacked TaB and Co-Fe-B amorphous layers in a magnetic tunnel junction (MTJ) to yield a higher magnetoresistance (MR) ratio and stronger synthetic anti-ferromagnetic (SAF) coupling. The technique yielded an ultra-smooth surface (Ra ∼ 0.1 nm) for both amorphous films and gave rise to atomically flat interfaces at the subsequently deposited layers. Top-pin MTJs fabricated with the technique exhibited superior properties, such as an MR ratio up to 315% and strong SAF coupling exceeding 0.7 erg cm-3. The smoothing process for amorphous layers will be an important for fabricating the MTJs of high-performance spintronics devices.