With an indirect band gap in the visible and a direct band gap at a much higher energy, boron phosphide (BP) holds promise as an unconventional p‐type transparent conductor. This work reports on reactive sputtering of amorphous BP films, their partial crystallization in a P‐containing annealing atmosphere, and extrinsic doping by C and Si. The highest hole concentration to date for p‐type BP (5 × 1020 cm−3) is achieved using C doping under B‐rich conditions. Furthermore, bipolar doping is confirmed to be feasible in BP. An anneal temperature of at least 1000 °C is necessary for crystallization and dopant activation. Hole mobilities are low and indirect optical transitions are stronger than that predicted by theory. Low crystalline quality probably plays a role in both cases. High figures of merit for transparent conductors might be achievable in extrinsically doped BP films with improved crystalline quality.
Unification of experiment and computation show how Mn alters the crystal and electronic band structure of the Ge1−xMnxTe alloy space. As a result, the effective mass is dramatically increased and the thermoelectric performance is improved.
6 June 2023 in Angewandte Chemie International Edition
AMX compounds with the ZrBeSi structure tolerate a vacancy concentration of up to 50 % on the M‐site in the planar MX‐layers. Here, we investigate the impact of vacancies on the thermal and electronic properties across the full EuCu1−xZn0.5xSb solid solution. The transition from a fully‐occupied honeycomb layer (EuCuSb) to one with a quarter of the atoms missing (EuZn0.5Sb) leads to non‐linear bond expansion in the honeycomb layer, increasing atomic displacement parameters on the M and Sb‐sites, and significant lattice softening. This, combined with a rapid increase in point defect scattering, causes the lattice thermal conductivity to decrease from 3 to 0.5 W mK−1 at 300 K. The effect of vacancies on the electronic properties is more nuanced; we see a small increase in effective mass, large increase in band gap, and decrease in carrier concentration. Ultimately, the maximum zT increases from 0.09 to 0.7 as we go from EuCuSb to EuZn0.5Sb.