Background: Since the combination of its rapid processing speed and high energy input, laser beam welding is considered advanced and suitable for welding thin and lightweight metals. The residual stresses deposited in the parts as a result of rapid heating and cooling render laserwelded components susceptible to fractures and deformities. Objective: In this patent, the modelling of the laser beam welding process during the joining of Ti- 6Al-4V and AA6061 dissimilar metals to analyze the effects of the welding process on residual stress and elastic strain by considering beam radius, beam offset, welding speed, and beam power as input parameters. Methods: The 3D model of the Ti-6Al-4V and AA6061 was developed using CATIA V5R16 software and beam radius. Beam offset, welding speed, and beam power are the input parameters considered, and the output parameters are stress and elastic strain. Design Expert is used to design the experiment. ANOVA was used, and a mathematical model was developed to analyze the performance characteristics of the welding process. Results: The results revealed that increasing the laser power increases residual stress, whereas it decreases with increasing the other parameters. The maximum average equivalent von Mises stress was 288.79 MPa, which is near the yield strength of AA6061. The optimum welding conditions selected for minimum possible residual stress is 1600.003 W, welding speed 0.05 m/s, beam radius 0.014 m. Conclusion: Based on the current observation during the simulation of joining dissimilar metals, the flow temperature along the weld line and weldment shows uneven distribution due to the dissimilarity of temperature-dependent properties of materials. The increased laser power leads to an increase in residual stress.
Although perovskite solar cells hold significant promise for next‐generation photovoltaic technologies, their development is hindered by challenges such as nonradiative recombination losses, limited scalability, and long‐term stability. To better understand the influence of device architecture and key fabrication parameters on photovoltaic performance, this study models and analyzes two widely adopted PSC structures—the inverted planar p–i–n and conventional n–i–p architectures—using the Solar Cell Capacitance Simulation One‐Dimensional (SCAPS‐1D) software. The effects of electron transport layer (ETL), hole transport layer (HTL), and perovskite layer thicknesses, as well as perovskite layer defect density, on the key photovoltaic parameters were systematically investigated. The results reveal that increasing the perovskite layer thickness and reducing defect density significantly improve the power conversion efficiency (PCE) of both structures. The p–i–n architecture achieved a higher PCE of 22.52% because of its improved fill factor (FF), whereas the n–i–p structure exhibited higher open‐circuit voltage (Voc) and short‐circuit current density (Jsc), resulting in a PCE of 21.07%. Reducing the defect density from 1E+16 (cm −3 ) to 1E+12 (cm −3 ) and increasing perovskite layer thickness from 500 nm to 800 nm increased the maximum PCE to 26.88% for the regular n–i–p PSC and 28.22% for the inverted p–i–n PSC. Overall, based on the theoretical analysis and comparison with experimental results reported by other researchers, the inverted p–i–n architecture emerges as a promising candidate because of its superior efficiency, lower hysteresis, and fabrication simplicity, although the selection of an effective HTL remains a significant challenge. These findings provide valuable insights for the design and optimization of efficient PSCs.