15 November 2017 in IEEE Transactions on Applied Superconductivity
A superconducting joint and a persistent current switch are the key technologies in persistent current operation for MRI and NMR magnets to obtain higher resolution and sensitivity. We prepared a persistent current system including a superconducting joint, a persistent current switch, and a double pancake coil, which were fabricated with a REBCO tape. The magnetic field decay behavior in persistent current operation were observed in a self-field and the external magnetic field of 1 T at 20 K. In the self-field, the decay rate of persistent current excited up to 170 A reached to 1.7 ppm/h after five days operation. This means that the practical persistent current operation has been achieved successfully using the REBCO superconducting joint. From the voltage-current characteristics estimated from the magnetic field decay, it was found that the decay behavior of persistent current is dominated by the joint resistance in 1 T, but by the shielding current in the self-field.
2 March 2023 in IEEE Transactions on Applied Superconductivity
The SCSC cable is a low-ac-loss, robust, and high-current cable concept, in which copper-plated multifilament coated conductors are wound spirally on a core. Its copper connecting filaments electrically improves the robustness against local defect and local normal transition. Its spirally geometry plays an equivalent role to the twist geometry of low T c superconductors in order to decouple filaments and, then, to reduce magnetization losses effectively. We fabricated four-layer SCSC cables with metal cores, which are preferable from the viewpoint of current sharing to help quench protection, but in which eddy current loss might be generated under ac magnetic fields. In order to examine the influence of metal cores on the magnetization losses, we measured the magnetization losses in SCSC cables, whose cores were twisted copper wires (twisted bundle of copper wires) and a GFRP rod, as well as those in various cores themselves. We fabricated four-layer SCSC cables whose core was twisted bare copper wires, and examined its current transport characteristics in liquid nitrogen.
27 April 2022 in IEEE Transactions on Applied Superconductivity
We can achieve both small magnetization loss and the robustness against local defect or local normal transition by winding copper-plated multifilament coated conductor spirally. The particular focus of this study is the impact of narrowing conductor (tape) width as well as filament width on magnetization losses. We measured the magnetization losses of various spiral copper-plated multifilament coated conductors, separated them into hysteresis losses and coupling losses, and examined the impact of narrowing filament width and conductor width. We demonstrated that the magnetization loss of the spiral 2 mm-wide coated conductor with 0.2 mm-wide filaments and 10 m-thick copper was one-twentieth of that of a flat standard 4 mm-wide coated conductor in transverse ac magnetic fields of 65.44 Hz.