This study investigates the hardened properties of mortar specimens produced by alkali-activated materials with ground granulated blast furnace slag (GGBFS) blended with waste red brick powder (WRBP). Three mixtures containing 40% red brick powder with water-to-solid ratios (w/s) of 0.35, 0.4 and 0.5 were designed, accompanied by a non-WRBP mixture with w/s of 0.4. The hardened properties were examined via compressive strength, ultrasonic pulse velocity (UPV), length change, and electrical surface resistivity (ESR) up to 28-day of curing age. The results illustrated that reusing WRBP slightly reduced the mechanical properties of mortar samples. Besides, increasing w/s ratio significantly mitigated the engineering properties of the specimens. At 28-day, the green mortar samples exhibited a good quality with high UPV values (>3660m/s), ESR values $(> 20\mathrm{k}\Omega-\text{cm})$ .