Olga Kashina

Olga Kashina

Auto-generated profile, based on publicly available information

Olga Kashina

Institute of Strength Physics and Materials Science, Siberian Branch of the Russian Academy of Science, 634055 Tomsk, Russia

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
17 June 2022 in Materials
Verified
Journal Article
Open access
PDF file
Aleksandr LotkovAleksandr Lotkov
Aleksandr Lotkov
VGVictor Grishkov
Victor Grishkov
Roman S. LaptevRoman S. Laptev
Roman S. Laptev
YMYuri P. Mironov
Yuri P. Mironov
DZDorzhima Zhapova
Dorzhima Zhapova
OKOlga Kashina
Olga Kashina
The experimental results regarding the effect of warm (573 K) abc pressing with an increase in the specified true strain, e, up to 9.55, on the microstructure and crystal structure defects (dislocations, vacancies) of the Ti49.8Ni50.2 (at %) alloy are presented. It is shown that all samples (regardless of e) have a two-level microstructure. The grains–subgrains of the submicrocrystalline scale level are in the volumes of large grains. The average sizes of both large grains and subgrain grains decrease with increasing e to 9.55 (from 27 to 12 µm and from 0.36 to 0.13 µm, respectively). All samples had a two-phase state (rhombohedral R and monoclinic B19′ martensitic phases) at 295 K. The full-profile analysis of X-ray reflections of the B2 phase obtained at 393 K shows that the dislocation density increases from 1014 m−2 to 1015 m−2 after pressing with e = 1.84 and reaches 2·1015 m−2 when e increases to 9.55. It has been established by positron annihilation lifetime spectroscopy that dislocations are the main type of defects in initial samples and the only type of defects in samples after abc pressing. The lifetime of positrons trapped by dislocations is 166 ps, and the intensity of this component increases from 83% in the initial samples to 99.4% after pressing with e = 9.55. The initial samples contain a component with a positron lifetime of 192 ps (intensity 16.4%), which corresponds to the presence of monovacancies in the nickel sublattice of the B2 phase (concentration ≈10−5). This component is absent in the positron lifetime spectra in the samples after pressing. The results of the analysis of the Doppler broadening spectroscopy correlate with the data obtained by the positron annihilation lifetime spectroscopy.

18 June 2022 in Metals
Verified
Journal Article
Open access
PDF file
Aleksandr LotkovAleksandr Lotkov
Aleksandr Lotkov
OKOleg Kashin
Oleg Kashin
VGVictor Grishkov
Victor Grishkov
DZDorzhima Zhapova
Dorzhima Zhapova
KKKonstantin Krukovskii
Konstantin Krukovskii
OKOlga Kashina
Olga Kashina
The mechanical properties of Ti49.8Ni50.2 (at %) alloy under tension at room temperature are studied in dependence on the true strain (e = 1.84–9.55) specified during isothermal multi-axial forging (abc-pressing). It was found that the stress at the beginning of the pseudoyield plateau does not depend on the value of the true abc-strain. It was found that after abs-pressing, already at a true strain e = 1.84, the yield stress σy was 900 ± 25 MPa, which is more than twice as high as compared to σy in the initial state of the specimens. With a further increase in the abc-strain, the yield stress continues to increase slightly and reaches 1000 ± 25 MPa at e = 9.55. In this case, the ultimate tensile strength of the samples increases by about 15%. The strain-hardening coefficient ϴ = dσ/dε at the III (linear) stage of the σ(ε) curve has a similar dependence on e. It is shown that after abc-pressing with e from 1.84 to 9.55, the yield stress and ultimate tensile increase linearly with increasing d−1/2 in accordance with the Hall–Petch relation, where d is the average grain–subgrain size.