6 May 2022 in Nuclear Fusion
ITER will operate with a tungsten divertor, a material featuring surface morphology changes when exposed to helium plasmas, in particular the formation of the so called tungsten fuzz under specific conditions. Investigating interactions between tungsten plasma facing components and helium plasmas in a tokamak environment is therefore a key point to consolidate predictions for the ITER divertor performance and lifetime. To this end, a dedicated helium campaign was performed in the full tungsten WEST tokamak, cumulating ∼2000 s of repetitive L mode discharges. It is shown that conditions for tungsten fuzz formation, as derived from linear devices experiments (incident helium energy E inc > 20 eV, helium fluence >1024 He/m2, surface temperature T surf > 700 °C), were met in the outer strike point (OSP) area of the inertially cooled tungsten divertor elements of WEST. Preliminary inspection of the components after the campaign did not show visible signs of surface modification, but points to significant net erosion in the OSP area. An extensive post mortem analysis is now ongoing to confirm these first indications. These results underline that the complex balance between erosion/redeposition (in particular linked to impurities) and tungsten fuzz formation needs to be taken into account in tokamak conditions.
23 September 2021 in Nuclear Fusion
TCThe Eurofusion Wp Pfc Contributors
The Eurofusion Wp Pfc Contributors
+20
23 November 2020 in Physical Review Letters
Erosion of material by energetic ions, i.e., sputtering, is widely used in industry and research. Using experiments and simulations that, independently of each other, obtain the sputter yield of thousands of individual grains, we demonstrate here that the sputter yield for heavy keV ions on metals changes as a continuous function of the crystal direction. Moreover, we show that polycrystalline metals with randomly oriented grains do not sputter with the same yield as the amorphous material. The key reason for this is attributed to linear collision sequences rather than channeling.
7 September 2021 in Physica Scripta
The net erosion and deposition patterns in the inner and outer divertor of WEST were determined after different experimental campaigns (C3 and C4) of the first operational phase using ion beam analyses and scanning electron microscopy techniques. The analyses were performed on four entire tiles from inertially cooled, W-coated divertor units with an additional Mo marker coating covered with a further W coating. Strong erosion occurred at the expected location of the inner and outer strike line area with a campaign-averaged net erosion rate of >0.1 nm s−1. On the high field side of the inner strike line area, thick deposited layers were found (>10 μm; growth rate >1 nm s−1), mainly composed of B, C, O, and W. Additionally, strong arcing was observed in this region. At the end of the C4 campaign, He discharges were performed to study the He-W interaction. Although the conditions for nanotendrils, i.e. fuzz formation were fulfilled around the outer strike line position, neither nanotendrils nor He bubbles (>10 nm) were observed at this area.
1 January 1996 in Journal of the Chemical Society, Faraday Transactions
Recent advances in electron energy loss spectroscopy are reviewed. After a short discussion of the principal limitations of energy loss spectrometers, the first results obtained with a recently designed spectrometer with angular aberration correction, are presented.
28 September 2021 in Physica Scripta