Constructing a LiF-rich solid electrolyte interphase (SEI) is a feasible strategy for inhibiting lithium (Li) dendrites of Li metal anodes (LMAs). However, selecting appropriate F-containing additives with efficient LiF contribution is still under active research. Herein, a series of fluorinated additives with diverse F/C molar ratios are investigated, and we demonstrate that the hexafluoroglutaric anhydride (F6−0) holds the best capability to derive the LiF-rich SEI in regular carbonate electrolytes (RCEs). To ameliorate the decomposition kinetics of the F6−0, LiNO3 (LNO) as an adjuvant is further introduced in the system. As a result, the reduction efficiency of F6−0 is increased to 91% under the F6−0/LNO synergistic effect, enabling the LMA with a uniform LiF-rich SEI in the RCE with merely 4 vol. % F6−0/LNO (F6L) addition. The LiNi0.8Co0.1Mn0.1O2||Li-20μm full-cell with the F6L also showcases better cycling and rate performances than the cases with other F-containing additives.
2 September 2016 in ACS Applied Materials & Interfaces
Crumpled microstructures enable reduction of reflection at the graphene surface and make crumpled graphene balls as excellent broadband light absorbers.
A functional coating layer (FCL) is widely applied in fast-charging lithium-ion batteries to improve the sluggish Li+ transport kinetics of traditional graphite anodes. However, blindly increasing the Li+ conductivity for FCL reduces the overall electron conductivity of the anodes. Herein, we decoupled the effect of La-doping on TiNb2O7 (TNO) in terms of the phase evolution, Li+/electron transport, and lithiation behavior, and then proposed a promising La0.1TNO FCL with balanced Li+/electron transport for a fast-charging graphite anode. By optimizing the doping concentration of La, more holes are introduced into the TNO as electron carriers without causing lattice distortion, thus maintaining the fast Li+ diffusion channel in TNO. As a result, the graphite with La0.1TNO FCL delivers an excellent capacity of 220.2 mAh g-1 (96.3% retention) after 450 cycles at 3 C, nearly twice that of the unmodified one.