8 May 2017 in Journal of Applied Physics
Verified
Journal Article
Open access
TNT. Niewelt
T. Niewelt
MSM. Selinger
M. Selinger
NGN. E. Grant
N. E. Grant
WKW. Kwapil
W. Kwapil
JMJ. D. Murphy
J. D. Murphy
MSM. C. Schubert
M. C. Schubert
In this paper, we present new insight in the degradation and subsequent recovery of charge carrier lifetime upon light soaking at 75 °C observed in float-zone silicon wafers. Variations of doping type, dielectric passivation schemes and thermal treatments after layer deposition were performed. The degradation was only observed for p-type float-zone silicon wafers passivated with passivation schemes involving silicon nitride layers. An influence of thermal treatments after deposition was found. N-type wafers did not degrade independent of their passivation scheme. Room temperature re-passivation experiments showed the degradation to affect the wafer bulk, and photoluminescence studies demonstrated fine lateral striations of effective lifetime. We conclude that the degradation is caused by bulk defects that might be related to hydrogen complexes.

10 October 2017 in Physica Status Solidi (RRL) – Rapid Research Letters
Verified
Journal Article
Open access
PDF file
NGNicholas Grant
Nicholas Grant
JMJohn D. Murphy
John D. Murphy
Accurate measurements of the bulk minority carrier lifetime in high‐quality silicon materials is challenging due to the influence of surface recombination. Conventional surface passivation processes such as thermal oxidation or dielectric deposition often modify the bulk lifetime significantly before measurement. Temporary surface passivation processes at room or very low temperatures enable a more accurate measurement of the true bulk lifetime, as they limit thermal reconfiguration of bulk defects and minimize bulk hydrogenation. In this article we review the state‐of‐the‐art for temporary passivation schemes, including liquid immersion passivation based upon acids, halogen‐alcohols and benzyl‐alcohols, and thin film passivation usually based on organic substances. We highlight how exceptional surface passivation (surface recombination velocity below 1 cm s−1) can be achieved by some types of temporary passivation. From an extensive review of available data in the literature, we find p‐type silicon can be best passivated by hydrofluoric acid containing solutions, with superacid‐based thin films showing a slight superiority in the n‐type case. We review the practical considerations associated with temporary passivation, including sample cleaning, passivation activation, and stability. We highlight examples of how temporary passivation can assist in the development of improved silicon materials for photovoltaic applications, and provide an outlook for the future of the field.

19 February 2021 in Solar RRL
Verified
Journal Article
Open access
PDF file
NGNicholas Grant
Nicholas Grant
PAPietro P. Altermatt
Pietro P. Altermatt
TNTim Niewelt
Tim Niewelt
RPRegina Post
Regina Post
WKWolfram Kwapil
Wolfram Kwapil
JMJohn D. Murphy
John D. Murphy
Czochralski‐grown gallium‐doped silicon wafers are now a mainstream substrate for commercial passivated emitter and rear cell (PERC) devices and allow retention of established processes while offering enhanced cell stability. We have assessed the carrier lifetime potential of such Czochralski‐grown wafers in dependence of resistivity, finding effective lifetimes well into the millisecond region without any gettering or hydrogenation processing, thus demonstrating one advantage over boron‐doped silicon. Second, the stability of gallium‐doped PERC cells are monitored under illumination (>3000 h in some cases) and anomalous behavior is detected. While some cells are stable, others exhibit a degradation then recovery, reminiscent of light and elevated temperature‐induced degradation (LeTID) observed in other silicon materials. Surprisingly, cells from one ingot exhibit LeTID‐like behavior when annealed at 300 °C but near stability when not annealed, but, for another ingot, the opposite is observed. Moreover, a stabilization process typically used to mitigate boron–oxygen degradation does not influence any cells that are studied. Secondary‐ion mass spectrometry of the PERC cells reveals significant concentrations of unintentionally incorporated boron in some cases. Nevertheless, even in the absence of mitigating light‐induced degradation, Ga‐doped silicon is still more stable than unstabilized B‐doped silicon under illumination.

3 October 2017 in IEEE Journal of Photovoltaics
Verified
Journal Article
Open access
NGNicholas Grant
Nicholas Grant
TNTim Niewelt
Tim Niewelt
NWNeil R. Wilson
Neil R. Wilson
EWEvangeline C. Wheeler-Jones
Evangeline C. Wheeler-Jones
JBJames Bullock
James Bullock
JMJohn D. Murphy
John D. Murphy
Minimizing carrier recombination at interfaces is of extreme importance in the development of high-efficiency photovoltaic devices and for bulk material characterization. Here, we investigate a temporary room temperature superacid-based passivation scheme, which provides surface recombination velocities below 1 cm/s, thus placing our passivation scheme amongst state-of-the-art dielectric films. Application of the technique to high-quality float-zone silicon allows the currently accepted intrinsic carrier lifetime limit to be reached and calls its current parameterization into doubt for 1 Ω·cm n-type wafers. The passivation also enables lifetimes up to 65 ms to be measured in high-resistivity Czochralski silicon, which, to our knowledge, is the highest ever measured in Czochralski-grown material. The passivation strategies developed in this work will help diagnose bulk lifetime degradation under solar cell processing conditions and also help quantify the electronic quality of new passivation schemes.

4 September 2022 in Advanced Materials Interfaces
Verified
Journal Article
Open access
SPSophie L. Pain
Sophie L. Pain
EKEdris Khorani
Edris Khorani
TNTim Niewelt
Tim Niewelt
AWAilish Wratten
Ailish Wratten
GFGalo J. Paez Fajardo
Galo J. Paez Fajardo
JMJohn D. Murphy
John D. Murphy
Surface passivating thin films are crucial for limiting the electrical losses during charge carrier collection in silicon photovoltaic devices. Certain dielectric coatings of more than 10 nm provide excellent surface passivation, and ultra‐thin (<2 nm) dielectric layers can serve as interlayers in passivating contacts. Here, ultra‐thin passivating films of SiO2, Al2O3, and HfO2 are created via plasma‐enhanced atomic layer deposition and annealing. It is found that thin negatively charged HfO2 layers exhibit excellent passivation properties—exceeding those of SiO2 and Al2O3—with 0.9 nm HfO2 annealed at 450 °C providing a surface recombination velocity of 18.6 cm s−1. The passivation quality is dependent on annealing temperature and layer thickness, and optimum passivation is achieved with HfO2 layers annealed at 450 °C measured to be 2.2–3.3 nm thick which give surface recombination velocities ≤2.5 cm s−1 and J0 values of ≈14 fA cm−2. The superior passivation quality of HfO2 nanolayers makes them a promising candidate for future passivating contacts in high‐efficiency silicon solar cells.

13 August 2020 in Nanoscale
Verified
Journal Article
Open access
PDF file
NGNicholas Grant
Nicholas Grant
APAlex I. Pointon
Alex I. Pointon
RJRichard Jefferies
Richard Jefferies
DHDaniel Hiller
Daniel Hiller
YHYisong Han
Yisong Han
JMJohn D. Murphy
John D. Murphy
Chemical treatments play an essential role in the formation of high quality interfaces between materials, including in semiconductor devices, and in the functionalisation of surfaces. We have investigated the effects of hydrogen and fluorine termination of (100)-orientation silicon surfaces over a range of length scales. At the centimetre scale, lifetime measurements show clean silicon surfaces can be temporarily passivated by a short treatment in both HF(2%) : HCl(2%) and HF(50%) solutions. The lifetime, and hence surface passivation, becomes better with immersion time in the former, and worse with immersion time in the latter. At the nanometre scale, X-ray photoelectron spectroscopy and atomic force microscopy show treatment with strong HF solutions results in a roughened fluorine-terminated surface. Subsequent superacid-derived surface passivation on different chemically treated surfaces shows considerably better passivation on surfaces treated with HF(2%) : HCl(2%) compared to HF. Lifetime data are modelled to understand the termination in terms of chemical and field effect passivation at the centimetre scale. Surfaces passivated with Al2O3 grown by atomic layer deposition behave similarly when either HF(2%) : HCl(2%) or HF(50%) are used as a pre-treatment, possibly because of the thin silicon dioxide interlayer which subsequently forms. Our study highlights that chemical pre-treatments can be extremely important in the creation of high quality functionalised surfaces.