Department of Mechanical Engineering (DAMEC) Universidade Tecnológica Federal do Paraná (UTFPR) Rua Deputado Heitor Alencar Furtado, 5000 Curitiba 81280‐340 PR Brazil
Auto-generated profile, based on publicly available information
Elisiane Maria Berton
Department of Mechanical Engineering (DAMEC) Universidade Tecnológica Federal do Paraná (UTFPR) Rua Deputado Heitor Alencar Furtado, 5000 Curitiba 81280‐340 PR Brazil
Samples of AISI 409 were thermochemically treated by the Solution Heat Treatment after Plasma Nitriding (SHTPN) process. SHTPN process consisted of a nitriding step followed by solution annealing at 1100 °C and rapid cooling down to room temperature. The second cycle of quenching (950 or 1050 °C), followed by tempering (250, 450, or 650 °C), was performed sequentially to SHTPN. Lubricated reciprocating tests were employed to analyze friction and wear behaviors. A bearing steel ball was used as a counterpart. The analysis of worn surfaces was assessed using optical interferometry and depth-sensing indentation. The last technique allows determining the work hardening caused by the wear process. Friction behavior was related to the deformation component: the higher the hardening, the higher the friction coefficient. Abrasion is the primary mechanism observed in all specimens, but there is a transitional behavior that depends on the original hardness of the surface. Samples with a similar hardness of bearing ball presented delaminated regions caused by highly deformed thin layer fatigue. Amongst SHTPN conditions NS-Q950-T2 and NS-Q1050-T2 presented the best balance of wear and corrosion performances.
Anais do Congresso Internacional de Engenharia Mecânica e Industrial (978-65-5941-094-1) - Avaliação Da Sensitização E Dureza Do Aço Inoxidável Martensítico Aisi 420 Tratado Por Têmpera E Revenido
This study presents a comparative analysis of the hardness and intergranular corrosion resistance of two types of martensite: nitrogen‐enriched martensite formed in AISI 409 ferritic stainless steel and carbon martensite of AISI 420 martensitic stainless steel. AISI 409 samples are treated by the solution heat treatment after plasma nitriding technique, quenching (1050 °C), and tempering (250, 350, 450, and 650 °C). AISI 420 samples are quenched and tempered at the same temperatures. Microstructure, hardness, intergranular corrosion resistance, and degree of sensitization (DOS) are evaluated using optical microscopy, Vickers microhardness, and double loop electrochemical potentiokinetic reactivation tests. The results shows a nitrogen martensitic layer whose thickness is over 750 μm on AISI 409. Concerning hardness, both materials exhibit a decrease as the tempering temperature increases. For the untreated and those tempered at 250 °C samples, both steels exhibit similar results. For the other temperatures, AISI 409 shows higher hardness only for the treatment at 450 °C. Regarding corrosion, carbon martensite exhibits a higher DOS in samples tempered at 250, 450, and 650 °C compared to nitrogen martensite. In the tempering condition at 350 °C, both materials shows a similar DOS. The best results are obtained by the AISI 409 tempered at 250 °C.