Hydrogen is one of the key elements for the economy based on renewable and sustainable resources. Because a very low concentration of hydrogen in metallic structural materials often causes hydrogen embrittlement and decreases their mechanical property, there is a great interest in the development of an inexpensive and versatile sensor for hydrogen in metals with high sensitivity and high spatial resolution. Here, real‐time visualization of atomic state hydrogen in a metal has been successfully achieved using a hydrogenochromic sensor consisting of a conventionally fabricated polyaniline layer and an interfacial Ni layer plated on the metal surface. The color change of the polyaniline layer due to its hydrogenation reaction can visualize the distribution of atomic state hydrogen in metals. Because the Ni interfacial layer functions as a catalyst for the hydrogenation reaction, the high sensitivity of ≈2 µmol m–2 and high spatial resolution of hundreds of micrometers are realized. This study opens a gate to a general approach for visualizing atomic state hydrogen in metals using polymers. In addition to the easy fabrication process and simple analytical method, the high sensitivity and high spatial resolution make the hydrogenochromic sensor promising for studying hydrogen behavior in metals.
10 January 2019 in Journal of the Electrochemical Society
The mechanism of trenching and pitting at intermetallic particles in AA1050 aluminum was investigated by open circuit potential measurements and microscopic polarization measurements, and the role played by the two types of intermetallic particles, Al-Fe and Al-Fe-Si, in this process was determined. Trenching was observed only around the Al-Fe-Si particles in the naturally aerated 0.1 M NaCl solution. Under the anodic polarization of AA1050 in naturally aerated 0.1 M NaCl, a crystallographic pit was initiated in the trench. However, neither trenching nor pitting occurred in the citric-citrate buffer with 0.1 M NaCl under naturally aerated conditions. Trenching was confirmed to be the result of the local alkalization induced by the oxygen reduction reaction on the particles. Micro-scale polarization showed that trenching occurred around the Al-Fe-Si particle from −0.9 to −0.6 V and did not occur above −0.5 V. While the surface of pure Al dissolved at pH 14 in 1 M NaCl, the corrosion morphology was different from pitting. Crystallographic pits occurred when the pure Al was immersed in 1 M NaCl at pH 0.0 after preimmersion in 1 M NaCl (pH 14). It was concluded that the change in local pH from alkaline to acidic triggers the morphological change from trenching to pitting.
The relationship between the change in the open-circuit potential (OCP) and the morphology of metastable pitting at Al–Fe–Si particles of AA1050 aluminum in 0.1 M NaCl was clarified. First, a metastable pit grew in the depth direction as the OCP decreased suddenly. Second, the pit started to grow on the Al surface, and the OCP remained low. Finally, the pit was repassivated with the reincrease of the OCP. In the early stage of OCP measurements of the electrode area of 1 cm2, the potential oscillations and values were found to be associated with the growth of many metastable pits rather than the initiation and repassivation of each metastable pit. The amplitude of the OCP oscillation decreased with time and disappeared. Then, the OCP decreased slowly and became constant. The transition from metastable to stable pitting was determined to occur gradually.
11 February 2024 in International Journal of Hydrogen Energy