14 February 2000 in Applied Physics Letters
and self-assembled quantum dots are fabricated on GaAs by gas-source molecular beam epitaxy. The effect of growth temperature on island density, island size, and optical properties is studied in detail. From a single layer of dots embedded in GaAs, peak photoluminescence wavelength of up to 1.52 μm is detected at room temperature. Thus, the fabrication of 1.3 and 1.55 μm GaInNAs quantum dot lasers on GaAs becomes feasible.
11 September 2000 in Applied Physics Letters
Electron effective mass in quantum wells (QWs) is investigated by the optically detected cyclotron resonance technique. The values of and are directly determined for the 70-Å-thick QWs with N composition of 1.2% and 2.0%, respectively. This sizable increase in the electron effective mass is consistent with the earlier theoretical predictions based on the strong interaction of the lowest conduction band states with the upper lying band states or impurity band induced by the incorporation of N.
5 February 2001 in Physical Review B
We perform a spectroscopic study on samples with N concentrations near an important value of an intermediate concentration between the impurity limit and the alloy region. We find that near samples exhibiting seemingly different spectra as reported in the literature and observed in our measurements actually have the same underlying electronic structure. Namely, the shallow N-induced bound states have already formed an impurity band and thus led to an observable band-gap reduction, but deeper N-related bound states persist as discrete levels below the newly formed band edge. The role of these discrete states in the formation of the new band edge on further increasing the N doping levels is discussed. We point out that although the nitrogen bound states form an impurity band in heavily N-doped GaAs, the states constituting such a newly formed band continue to retain certain localization characteristics of the impurity in the dilute limit. We observe that the impurity band gives rise to strong resonant Raman scattering, which makes it possible to obtain the resonant Raman profile near the direct band edge of this direct-gap semiconductor.
27 August 1999 in Applied Physics Letters
P-type, Be-doped GaInNAs layers (1100 Å thick) are grown on GaAs substrates by gas-source molecular beam epitaxy with a nitrogen radical beam source. High-resolution x-ray rocking curves show that the peak shifts closer to the GaAs substrate peak with increasing N concentration, indicating reduced strain. After rapid thermal annealing (RTA) at 700 °C for 10 s, the sample suffers strain relaxation, but the N-containing samples remain pseudomorphically strained, suggesting better thermal stability of GaInNAs. The wavelength of room-temperature photoluminescence redshifts from 0.988 to 1.276 μm, due to large band gap bowing, with N concentration increased from 0 to 0.024. Secondary ion mass spectrometry results show no Be diffusion, but hydrogen incorporation alongside N. The free carrier concentration is decreased by one order of magnitude mainly due to H passivation, but after RTA at 700 °C, it is increased to half that of GaInAs due to the reduced H concentration. The product of carrier concentration and Hall mobility is increased from one-tenth to about half that of the GaInAs sample.
4 March 2002 in Applied Physics Letters
Based on the results of temperature-dependent photoluminescence (PL) and absorption measurements, the PL emission in GaNP epilayers and GaNP/GaP multiple quantum well structures with N composition up to 4% is shown to be dominated by optical transitions within deep states likely related to N clusters. With increasing N composition, these states are shown to become resonant with conduction band of the alloy and thus optically inactive, leading to the apparent redshift of the PL maximum position.
2 January 2001 in Physical Review B
The first experimental signature of an intrinsic defect in GaNAs is provided from an optically detected magnetic resonance study. The resolved central hyperfine structure identifies the defect with a nuclear spin containing either an antisite or a Ga interstitial. From the strength of the hyperfine interaction and the growth conditions, a complex involving the antisite seems to be a more likely candidate.