This work describes the design, construction and testing of a continuous casting device coupled to an electromagnetic stirring system for the production of thixoforming feedstock using Al-Si alloys. The following processing and construction parameters were tested: pouring temperature (660-800 °C), mould cavity roughness (Ra = 0.17-1.06 µm), casting speed (2-4 mm/s), use of a combined (primary and secondary) cooling system and the intensity and radial penetration of electromagnetic stirring (0, 1500 and 3000 W stator power). The macro-appearance of the ingots and the longitudinal and radial microstructural parameters were then evaluated. The results indicate that the surface finish of the mould cavity was an important construction parameter as it had a strong influence on heat transfer and, consequently, feed speed; use of a secondary cooling system for the mould allowed greater grain refinement and microstructural homogeneity to be achieved for all the conditions tested; optimal electromagnetic stirring power was 1500 W (EMFmax = 22 Gauss); this resulted in a grain size-to-dendritic arm spacing ratio of close to 1, which is suitable for subsequent SSM processing.
24 April 2025 in Journal of Materials Engineering and Performance
This article studies the fatigue behavior of the Al-5wt%Si-2.5wt%Cu alloy. The effect of combining techniques of chemical grain refining (Al-5wt%Ti-1wt%B alloy) added to electromagnetic stirring, CGR+EMS, is demonstrated in this work. This combination produced a microstructure with reduced grain size (121 ± 20 µm) when compared with the raw material produced only by electromagnetic stirring, EMS, (213 ± 38µm), with grain refiner Only, CGR, (184 ± 23 µm) or Without any Grain Refining Technique (WGRT) (413 ± 96 µm). The condition produced by associating electromagnetic stirring with the Al-5wt%Ti-1wt%B grain refiner presented the smallest grain size and less porosity. Thus, conditions CGR+EMS and WGRT were chosen to continue the evaluation of the mechanical performance of the studied alloy via tensile tests, whose results for ultimate tensile stress, yield strength and elongation were, respectively, WGRT/ CGR+EMS, UTS = 160.3 ± 9.5 / 208 ± 10 MPa, YS (0.2%) = 110 ± 2 / 135 ± 3.5 MPa and ε(%) =3.2 ± 0.1 / 2.9 ± 0.1. Fatigue tests were conducted via the staircase method. The average estimate of fatigue strength for a given life (107 cycles) and the standard deviation calculated for WGRT and CGR+EMS condition were, respectively, = 60.1 MPa / 71.6 MPa and = 3.30 / 6.42.