30 June 2020 in Polytechnic Journal
The aim of this study is to investigate the influence of different heat inputs on mechanical properties and microstructure of dissimilar electrical arc welded austenitic stainless steel AISI 304 and low-carbon steel (CS) joints. The mechanical properties of welded austenitic stainless steel type AISI 304 and low-CS are studied. Five different heat inputs 0.5, 0.9, 1.41, 2, and 2.5 KJ/min were applied to investigate the microstructure of the welded zone and mechanical properties. The results showed that the efficiency of the joints and tensile strength increased with increasing heat inputs, while excess heat input reduces the efficiency. Furthermore, changes in microstructure with excess heat input cause failure at the heat-affected zone.
24 January 2023 in Advances in Materials Science and Engineering
This study aims to detect the impact of preexfoliation corrosion on the efficiency of 2mm thick 2024-T3 aluminum alloy friction stir spot welded (FSSW) joints. Five specimens of FSSW joints, welded with 620rmin−1 rotational speed and a dwell time of 10seconds, were immersed in an exfoliation corrosion solution for five different times: 10h, 20h, 30h, 40h, and 50h. The tensile shear load for the noncorroded joint was 3.5kN. The results showed that the degradation of mechanical properties increased with increasing exposure time, and the joint efficiency drop reached 62 for specimens exposed for 50h to the corroded solution. As welded FSSW 2024-T3 AA joints exhibited a nugget debonding failure mode and a mixed-mode tensile-shear fracture, in the corroded specimens, only a shear fracture could be seen. The results were attributed to a reduction in the bonding area between the upper and lower sheets due to corrosion.
30 September 2025 in Zanin Journal of Science and Engineering
Super duplex stainless steel has strong mechanical properties and performance. The demand for this material in various industries in the world of engineering has increased due to its reliability. This material has been considered as an alternative to high alloy steel and other grades of stainless steel for their good technical and economic benefits. The performance comes from the structure of the material that consists of approximately equal rates of ferrite and austenite. However, this ratio and the material's structure can be influenced by production activities, such as the welding process. The level of degradation of properties can be reduced or prevented by utilizing the solid-state welding process due to its reduced heat input, thermal cycle, and absence of melting and recrystallization. Rotary friction welding is a solid-state welding process that can serve as an alternative to fusion welding, reducing and preventing the formation of undesired phases. In this study, the effect of rotary friction welding process parameters on microstructure and mechanical properties has been investigated. Different friction forces and forging forces are used to weld super duplex stainless-steel pipes. An acceptable result has been achieved, as the efficiency of the welded joint for the best case exceeds 100%. The ultimate tensile strength in this case is 928 MPa, surpassing the strength of the base material. The microstructure of the welded samples shows a good result for this welding process, so it can be considered for joining super duplex stainless steel to improve joint efficiency.
1 September 2025 in Al-Rafidain Engineering Journal (AREJ)
Rotary friction welding (RFW) is one of the most effective and efficient methods of joining for welding similar and dissimilar materials in different industrial applications. In this study, the influence of friction pressure of Continuous Drive Rotary Friction Welding (CDRFW) was investigated for welding austenitic stainless-steel pipe (grade TP316L) at two different friction times, while other welding process parameters remained constant during the process. The results demonstrate a complex relationship between the friction welding parameters. For the first set of samples with a longer period of friction time of 45 seconds, increasing the friction pressure decreases the mechanical properties. In contrast, for a shorter period of friction time of 15 seconds, increasing the friction pressure increases the mechanical properties. The best result among the welded samples was achieved at the highest friction pressure and the shorter friction time, with the tensile strength reaching 457 MPa. However, for the longer period of friction time of 45 seconds, the tensile strength is dropped to a minimum of 171 MPa. The key parameter in this process is the heat input, which must be carefully controlled. Excessive or insufficient heat input can lead to improper bonding and poor weld quality. The findings of this study show that welded joints with the highest friction pressure combined with lower friction time give the best result of tensile strength and hardness profile. In contrast, the high friction pressure and friction time together need to be avoided to prevent degraded weld performance.