Silicide – aluminide composites could be considered as potential tool materials, because of high wear resistance and thermal stability. Recently, the alloys based on iron aluminide and silicide were tested, but they found to be very brit...
27 October 2026 in Materials Science and Engineering: A
This research investigates the high-temperature interactions between Ni–Fe–Co–Cr and Ni–Fe–Co–Cr–Ti–Al high-entropy alloys and industrial ceramic refractories with high corundum (Al 2 O 3 ) content (approximately 68–85 wt%) and SiO 2 as a secondary component. The primary objective is to assess wettability quantitatively and elucidate interfacial reactions that led to the formation of reaction layers, non-metallic inclusions, and surface contamination during melting and casting. Sessile-drop wetting experiments were conducted using a CLASIC high-temperature observation furnace/heating microscope, capable of operating at temperatures up to 1600°C. Contact angles were evaluated using axisymmetric drop shape analysis. To mitigate oxidation and isolate interactions between the refractory materials and metals, the experiments were conducted either in a vacuum or under a controlled overpressure of ultra-high-purity argon (≥ 99.9999%). Post-experimental analysis of the metal–ceramic interfaces was performed using scanning electron microscopy with EDX microanalysis, along with X-ray powder diffraction, to examine interfacial morphology, elemental distribution, and reaction products. The comprehensive wetting and post-mortem characterizations revealed a direct correlation between composition-dependent wettability and the development of interfacial reaction layers or phases. The findings provide essential guidelines for selecting corundum-rich crucibles and molds, as well as for establishing processing parameters that minimize interfacial degradation, ultimately enhancing casting yield and the reliability of components.
Fe–Si–Ni–Al-based in-situ composites were synthesized using vacuum induction melting followed by centrifugal casting. The resulting microstructures exhibited characteristic features of in-situ composites, with FeSi forming directly during solidification and acting as the primary reinforcing phase within a NiAl-based matrix. In the as-cast state, the microstructure and phase composition were heterogeneous, and metastable ternary phases, including AlNi₂Si and Al₂FeSi, were identified. Heat treatment promoted chemical homogenization and phase stabilization, leading to the transformation of metastable phases into a stable two-phase microstructure composed of FeSi and NiAl. The microstructural evolution was found to depend strongly on the FeSi:NiAl ratio, corresponding to different regimes within a pseudobinary FeSi–NiAl system. Microhardness showed a strong dependence on FeSi content, with maximum values exceeding 1100 HV0.1 for FeSi-rich compositions. Tribological behavior was governed by a combination of abrasive and adhesive wear mechanisms, with improved wear resistance observed after heat treatment in FeSi-rich alloys. The mechanical and tribological properties of the cast composites were comparable to those of high-performance tool steel Vanadis 6. These results demonstrate that FeSi–NiAl in-situ composites prepared by casting can achieve competitive performance with powder metallurgy-derived materials, while offering advantages in terms of processing simplicity and scalability.