6 March 2021 in Packaging Technology and Science
Seal area represents the most problematic part in food packaging for controlling the moisture and gas ingress and preserving product quality. Understanding the mechanism of heat sealing, which is a widely used method in flexible packaging, is critical for maintaining product quality throughout the storage and preventing food waste. Likewise, understanding the factors causing the leak formation in the seal interface helps to avoid failures and increase integrity for all seal types produced by heat sealing methods. This review looks at heat sealing and its mechanisms in flexible food packaging materials and particularly focuses on the reasons behind the encountered seal integrity problems that have a detrimental effect on food quality and shelf life. Heat sealing mechanisms, form fill seal systems and seal types were analyzed. Then, factors affecting the leak formation have been grouped as process parameters, material properties, contaminants, and further processes, which is uncharted territory in open literature. Finally, the details of these groups and their interrelationships were examined and discussed. Revealed key factors as shown in this study are expected to guide future research for understanding leak formation mechanisms in flexible food packaging.
1 September 2021 in Food Packaging and Shelf Life
17 March 2021 in Packaging Technology and Science
Seal strength is a key indicator of heat seal quality in flexible packaging. In this study, the effect of seal bar geometry, material composition and food particle contamination on the seal strength of widely used low‐density polyethylene (LDPE)‐based compound films was examined. Additionally, the maximum level of allowable solid food particle contamination was determined for ground coffee particles and powdered sugar. The results showed that adding metallocene LLDPE compound decreases seal initiation temperature (SIT) and increases overall seal strength. Also, changing seal bar geometry from flat to grooved bar with 0.56‐mm pitch height enhanced the seal strength significantly. Moreover, pressure mapping and T‐peel tests at SIT pointed out that grooved bars alter the pressure distribution and first contact points through the seal surface. Contamination of ground coffee particles at the seal interface as occurs during the packaging process when a powdery product is dropped in a package did not affect the seal strength up to 10 g/m2 at 0.5‐s dwell time. Above that amount, seal strength dropped dramatically. In the case of powdered sugar, threshold contaminant level was 2 g/m2 at 0.5‐s dwell time. Consequently, it has been revealed that knowing the type and the amount of contaminant during the food packaging process is important to maintain the seal quality, to find optimum process values between dosing and filling and to choose the right seal bar design because they can have a critical influence, especially at seal initiation phase.
26 January 2023 in Packaging Technology and Science
Dwell time is one of the main parameters influencing heat seal quality and process efficiency in flexible packaging. In this study, the rheological behaviour of polypropylene (PP)/low‐density polyethylene (PE‐LD)‐based compound films containing different ratios of talc was examined. The minimum dwell time required to supply a sufficient sealing was estimated based on heat conduction time and reptation time. Reptation is a rheological concept used to described the behaviour of a polymer melt, and the reptation time is the time required for a molecule to escape from its surrounded entangled structure. The results showed that increased levels of talc are associated with elevated complex viscosities, storage and loss modulus as well as an increased seal strength. The estimated minimum required dwell time at the seal initiation temperature (SIT) dropped sharply with the initial introduction of 10 wt% talc. However, increasing the talc ratio to 30 wt% did not create any major change in the estimated time value. Also, observed T‐peel strength values for 0.1 and 0.5 s dwell time at SIT confirmed the predicted minimum required dwell time values. On the other hand, when the seal temperature is increased to the higher end of the operation window, time estimations did not match with the observed seal strengths. Here, the melting already starts and the molecules diffuse up to a certain distance before the interface temperature reaches the desired level. Recalculation of the average diffusion distance by including this pre‐melting situation can present a better approach for the temperatures above SIT. When the molecules diffused around halfway along the sealant thickness observed, seal strengths reached a sufficient level (2.5 N/25 mm) for both SIT and the highest end of the operation window. In conclusion, it has been revealed that knowing the reptation time and the required time for the heat conduction during the sealing process can help to predict the minimum required dwell time to achieve quality sealing, especially at low sealing temperatures. Additional surface characterizations also helped to elaborate on the influence of changing insoluble filler ratio on the seal initiation properties. It has been showed that the added talc increases the surface free energy and supplies easier wetting at the seal interface. Therefore, adding talc or a similar insoluble filler can help to make the heat sealing process more efficient.
11 October 2022 in Packaging Technology and Science
25 July 2026 in Packaging Technology and Science
Adding recycled content is paramount for achieving circular packaging. However, packaging films produced from postindustry or postconsumer recycled polyethylene (PCR PE) have been reported to have various visual and mechanical issues related to impurities and degradation, which affect their performance. This paper studies the gel presence and seal characteristics of packaging films produced from 100% monolayer PCR PE with the addition of antioxidants and compatibilizers. It additionally evaluates the performance of commercially produced multilayer PE films that contain 30% and 50% PCR PE in the core layers and virgin sealant and top layers, checking the quality variations that arise from the difference in PCR PE batches. In the research, the presence and surface area ratio of gels related to recycled content are analyzed using FTIR, microscopy and a newly introduced image analysis method; seal performance is measured via hot‐tack and cold‐tack tests, and material performance is evaluated via tensile testing. According FTIR findings, some spherical and fibre like impurities coming from PCR PE were found to be polyamide or cellulose based, respectively. In nonfood contact commercial films with PCR PE content, the quality varied largely from batch to batch as well as the hot and cold seal strength. In 100% PCR PE films produced in laboratory settings, adding antioxidants during film production did not significantly influence the gel presence while one of the maleic anhydride‐based (MAH) compatibilizers used in the research reduced both the gel number (from 432 to 375 pcs/9 cm 2 ) and gel area ratio (from 0.81% to 0.67%). On the other hand, both types of additives delayed the breakage failure providing a larger operation window in hot‐tack tests. During the cold‐tack test, stronger attachment at the seal interphase is observed at 100°C sealing temperature in samples with added compatibilizer. Finally, according to tensile test results, the Young's modulus and the elongation at break only showed slight changes with the addition of antioxidants and compatibilizers. The results can be used for guidelines for design from recycling working with PE films.