Department of Agroindustrial Technology, Faculty of Agricultural Technology, Gadjah Mada University, Jl Flora No 1 Bulaksumur, Yogyakarta, 55281, Indonesia, ugm.ac.id
Auto-generated profile, based on publicly available information
Wagiman Wagiman
Department of Agroindustrial Technology, Faculty of Agricultural Technology, Gadjah Mada University, Jl Flora No 1 Bulaksumur, Yogyakarta, 55281, Indonesia, ugm.ac.id
Oil palm empty fruit bunches (OPEFB) are lignocellulosic materials that are a by-product of the palm oil industry, which have less use and utilization is still limited. OPEFBs high cellulose content could potentially develop into various bioproducts, especially biomaterials. The thermochemical delignification process can obtain high-yieldalpha-cellulose. The cellulose extraction process can be done by combining the bleaching process under acidic conditions and alkaline delignification to obtain high-purity cellulose. The bleaching conditions vary in the concentration of NaClO2, the length of bleaching, the temperature, and the number of stages. The research obtains high α-cellulose by optimizing bleaching conditions under acidic conditions in celluloses OPEFB extraction with variability on NaClO2 concentration and bleaching time using response surface methodology (RSM). The bleaching process was implemented at an early stage with a concentration of 3 NaClO2 and a bleaching time of 2hours as a center point with a bleaching cycle of twice at pH 44.5 using acetic acid. Bleached fibers were delignified using 10 NaOH for 2hours at room temperature. The RSM analysis resulted in optimum bleaching conditions at a concentration of 3.22 NaClO2 for 1hour, yielding OPEFBs cellulose of 82.96±2.53, hemicellulose of 9.27±2.28, and lignin of 1.68±0.58. The validation and verification process in the bleaching conditions obtained cellulose of 84.87 and α-cellulose of 88.51, with a crystallinity index of 70.55 and crystallite size of 2.35nm. Scanning electron microscopy on surface cellulose morphology at optimum bleaching helped remove hemicellulose impurities, lignin, and inorganic materials and a more intensive opening of cellulose fibrils. The bleaching process optimization point was verified to improve the delignification performance and potentially produce high yield α-cellulose content for microcrystalline cellulose use.
1 January 2024 in International Journal of Chemical Engineering
Carboxymethyl cellulose (CMC), a water‐soluble cellulose, can be derived from oil palm empty fruit bunches (OPEFBs). In addition to being highly soluble, it is essential for CMC to exhibit excellent thermal stability when utilized in biocomposites. Reactants in the alkalization and etherification steps to provide high DS of CMC‐based OPEFB have not been standardized. The research aimed to optimize the alkalization and etherification processes using a response surface methodology (RSM). This will help in determining the optimal ratios of 30% NaOH (the center point of 3), isopropanol (the center point of 30) as maceration media, and monochloroacetic acid (the center point of 1.2) needed for the cellulose. RSM determined the optimum ratio of 30% NaOH to OPEFB cellulose, which was 3.36 : 1, an isopropanol ratio of 30.62 : 1, and an MCA to cellulose ratio of 1.19 : 1. The optimization indicates that the OPEFB cellulose‐based CMC have a high degree of substitution of 1.28 and a carboxymethyl content of 31.93%. CMC morphology showed noticeable changes, such as a smoother surface and swelling. There was a significant increase in the wavenumber of 1580 cm−1 due to the presence of carbonyl groups. The OPEFB‐based CMC resulted in a crystallinity of 40.18%, and thermal gravimetric analysis indicated that mass decreases occurred at high temperatures of 500°C, which suggests that the optimal CMC has a high thermal stability. OPEFB‐based CMC exhibits a high degree of substitution and resistance to thermal degradation, which makes it suitable for further use as the main material in biocomposite films.
1 January 2026 in International Journal of Biomaterials
Cellulose‐based hydrogel films are promising alternatives to plastic for wrapping. Hydrogel films based on carboxymethyl cellulose (CMC) and microcrystalline cellulose (MCC) must exhibit high mechanical strength and be capable of absorbing moisture. Crosslinking increases the absorption capacity and mechanical strength of hydrogel films. As a filler, MCC can synergize with citric acid, which acts as an environmentally friendly crosslinker to enhance mechanical strength. This research aimed to develop a suitable CMC/MCC formulation and citric acid as a crosslinker, resulting in a hydrogel with high water absorption and mechanical strength. CMC/MCC formulations were combined with citric acid concentrations of 5%, 7.5%, and 10%. The results showed that the MCC and citric acid will affect absorption and mechanical strength. The addition of MCC up to 50% tends to produce a brittle hydrogel film, and this phenomenon is also correlated with increased citric acid. A 90:10 CMC/MCC formulation with 5% citric acid (w/v) resulted in a water uptake of 222.72 ± 9.32 at pH 7.0. In contrast, the 80:20 CMC/MCC formulation resulted in a water uptake of 603.02 ± 26.98. They both showed higher rehydration of the dry gel than the others. FTIR confirmed the sharpening of the peak wave number at 1705 cm −1 , which is identical to the protonated carbonyl group and correlates with the water absorption capacity. The morphology of hydrogel films containing a CMC/MCC ratio of 90:10 exhibits a smoother surface than that of those with a CMC/MCC ratio of 80:20, which feature bubbles on the surface cracks of the hydrogel film due to the presence of more water absorption channels. Hydrogel films with a CMC/MCC ratio of 90:10 and 5% citric acid (w/v) can be developed for wrapping by modifying their hygroscopic properties. In contrast, hydrogel films with an 80:20 ratio and 5% citric acid are suitable for use as absorbents.