In this Letter, a high-pressure annealing (HPA) process is proposed as a way to reduce the thermal budget of Hf0.5Zr0.5O2 (HZO) thin films with ferroelectric behaviors. The low-thermal-budget process is essential for integrating ferroelectric devices in the back-end-of-line to provide more functionalities and effective memory area. For the HZO film annealed at 300 °C using the HPA process, an orthorhombic phase responsible for ferroelectric behavior was formed with a decrease in film thickness, resulting in a remanent polarization (Pr) of ∼13 μC/cm2 (i.e., 2Pr of ∼26 μC/cm2). Meanwhile, when only the annealing time was increased at 300 °C without applying pressure, the HZO film did not crystallize and exhibited linear dielectric properties. Consequently, the HZO films (<10 nm) can be crystallized by applying pressure (15 atm) even at low temperatures of 300 °C, thereby obtaining ferroelectric properties.
In this paper, we investigate the polarization retention of Hf0.5Zr0.5O2 (HZO)-based metal–ferroelectric–insulator–Si (MFIS) capacitors with scaling of the ferroelectric (FE) layer thickness from 5 nm to 20 nm. The capacitors have a constant interface layer capacitance of ∼24 μF/cm2, developed due to the integration of HZO on a degenerated Si as a bottom conducting electrode. It is observed that 20 nm HZO films show a small change (∼5%) in FE polarization (PFE) between short (10 μs) and long (6 s) retention time, while 5-nm-thick films exhibit a large difference (∼90%). The dependence of PFE retention loss on the FE thickness can be understood by the presence of a built-in electric field in the FE layer, generated due to charge continuity between the FE and the interface layers in the ground state without any external bias. A direct experimental observation also confirms that a residual voltage is developed at the node between the metal–ferroelectric–metal and metal–oxide–semiconductor capacitors connected in series, in the ground state with zero external bias. It is expected that a proper understanding of the built-in field developed in the FE layer in an MFIS stack is crucial for FE memory retention characteristics.
The ferroelectricity of metal–ferroelectric–metal capacitors with a ferroelectric HfxZr1−xO2/ZrO2 (HZO/ZO) bilayer thicker than 20 nm formed by atomic layer deposition and postdeposition annealing at 600 °C was investigated. The HZO/ZO capacitors exhibited a higher remanent polarization (2Pr = Pr+ − Pr−) and breakdown voltage (Vbd) than capacitors with a HfxZr1−xO2 (HZO) single layer. In particular, a HZO (15 nm)/ZO(10 nm) (HZ15Z10) capacitor exhibited excellent Vbd and 2Pr values of 6.7 V and 14 μC/cm2, respectively, which are much higher than those (4.3 V and 10 μC/cm2, respectively) for a HZO (15 nm) (HZ15) capacitor. The HZ15Z10 capacitor also exhibited higher endurance, a smaller wake-up effect (∼5%), and superior fatigue properties up to 108 switching cycles, compared to a HZ15 capacitor, which exhibited a large wake-up effect (∼15%) and large 2Pr degradation at 108 cycles. The wake-up behavior is attributed to domain depinning mainly related to the redistribution of oxygen vacancies and transformation from the nonferroelectric phase to the ferroelectric orthorhombic (O) phase during field cycling. The HZO/ZO bilayer grew a larger grain size with the ZO nucleation layer, which is twice as large as that of the HZO single layer, and the former structure exhibited more stable bulk-like ferroelectricity. Although the ferroelectric O phase in HZO decreased with increasing HZO thickness, the HZO/ZO structure had a larger fraction of the O phase than the HZO structure. Considering the manufacturing process of ferroelectric devices, these thick HZO/ZO bilayers are promising ferroelectric materials.
17 January 2019 in ACS Applied Materials & Interfaces
The change in the interplanar spacing (d-spacing) including the ferroelectric orthorhombic (O) phase in the low-temperature fabricated HfxZr1−xO2 (HZO) films was studied using synchrotron grazing-incidence wide-angle x-ray scattering analysis. The 10-nm-thick HZO films were fabricated by thermal and plasma-enhanced atomic layer deposition (TH- and PE-ALD) methods using H2O gas and O2 plasma as oxidants, respectively, and a post-metallization annealing (PMA) was performed at 300–400 °C. The d-spacing of the mixture of (111)-, (101)-, and (111)-planes of O, tetragonal (T), and cubic (C) phases, respectively, for the TH- and PE-ALD HZO films increased up to 2.99 Å with an increase in PMA temperature, while the d-spacing estimated by conventional x-ray diffraction was 2.92 Å regardless of the PMA temperature. The remanent polarization (2Pr= Pr+ − Pr−) of the HZO films increased as the PMA temperature increased. It is clear that the 2Pr value satisfied a linear relationship as a function of the d-spacing of O(111)/T(101)/C(111) phases. Furthermore, the wake-up effect was found to depend on the ferroelectric O phase formation. The wake-up effect was significantly reduced in both the TH- and PE-ALD HZO films after the PMA at 400 °C due to the increase in the ferroelectric O phase formation. The leakage current density (J)–electric field properties of the PE-ALD HZO film with the lowest d-spacing were divided into three steps, such as low, middle, and large J values, in the wake-up (103 cycles), pristine (100 cycle), and fatigue (107 cycles) states, respectively. Therefore, an analysis of the ferroelectric O phase is very important for understanding the ferroelectricity including endurance.
In this letter, a threshold switching (TS) selector with Ag doping-based nano-polycrystalline ZnO switching layer (SL) having (002) preferred orientation has been manifested, without incorporating an active Ag metal layer, using a facile co-sputtering deposition technique. The TS selectors with extremely controlled doping of ~0.14 at. % Ag concentration showed remarkable electroforming (EF)-free selection behavior such as gigantic selectivity (~10 11 ), extreme-low off -current (~10 fA), high on -current density (~1.6 MA/cm 2 ), ultra-steep switching slope (~0.8 mV/decade), satisfactory endurance (>10 6 ), fast switch- on speed (~38 ns) and relaxation speed (~64 ns), and high device yield (~90%). Furthermore, selector devices showed reproducible selection behavior with stable threshold voltage (V th ) having merely ~8% variances.