22 August 2022 in IEEE Transactions on Power Electronics
Due to their superior material properties, wide bandgap (WBG) semiconductors enable the application of power electronics at higher temperature operation, higher frequencies, and higher efficiencies compared to silicon (Si). However, the commonly-used aluminum wire bonding as topside interconnection technology prevents WBG semiconductors from reaching their full potential, due to inherent parasitic inductances, large size, heat dissipation, and reliability issues of wire bonding technology. Therefore, this article presents a comprehensive review of topside interconnection technologies of WBG semiconductor power devices and modules. First, the challenges and driving factors for the interconnection of WBG semiconductor dies are discussed. Second, for each widely commercially used WBG semiconductor, i.e., silicon carbide and gallium nitride, technical details and innovative features of state-of-the-art interconnection techniques in packages are reviewed. Then, the majority of existing topside interconnection materials for WBG semiconductors are categorized and compared, followed by a discussion of their advantages, challenges, and failure modes. Based on this elaborate discussion, potential future directions of the interconnection technology development are given. It is concluded that the superior performance of WBG semiconductors can be obtained by combining novel materials with innovative designs for the topside interconnections.
1 February 2011 in Journal of Physics: Conference Series
4 February 2025 in IEEE Transactions on Components, Packaging and Manufacturing Technology
Embedded packaging of wide bandgap power modules offers an inherently lower parasitic inductance, higher switching frequency and lower power losses compared to traditional wire-bonding technology. However, the present embedded technology suffers from a relatively tight laser drilling process window and unknown reliability. This work presents a new embedded packaging technology with minimal thermo-mechanical interfacial stress and a relaxed process window. For this purpose, a pre-sintered die top system (DTS) layer for an improved laser drilling process window with minimal interfacial stress in the topside interconnection is adopted. To design and fabricate the proposed new embedded power module, the interaction between different ceramics and the lamination resin is also studied. Furthermore, the thermal and thermomechanical stress characteristics of the proposed embedded, conventional embedded and wire-bonded power modules have been analyzed and compared through FEM multiphysics simulations in order to evaluate the performance of the three packaging approaches. The simulations indicate that despite the maximum von Mises stress of silicon-nitride (Si3N4) is the highest compared to its substrate counterparts, the obtained maximum stress is much lower than its flexural strength and thus is the best choice of substrate material. The silicon-carbide (SiC) module prototypes fabricated based on the proposed embedding technique show a good laser drilling performance, resulting in an excellent plating quality. In addition, our fabrication results show good agreement with the out-of-plane deformation simulation results. Finally, the proposed module exhibits good reproducibility and process stability due to the protection of the DTS layer.
1 September 2013 in Chinese Physics B
24 March 2025 in IEEE Transactions on Device and Materials Reliability
Silver (Ag) sintering is becoming more critical for future wide bandgap (WBG) power module substrate attachments. However, sintered Ag joints with plated aluminum (Al) heatsinks and directly bonded aluminum (DBA) substrates presently suffer from poor reliability. To resolve this problem, this work studies the reliability of plated (Nickel) Ni/Ag metallization on Al for sintered Ag joints and proposes a new plated Ni/Copper (Cu)/Ag metallization stack for improved reliability. The shear strength and thermal shock (TS) reliability of the sintered Ag joints for different metallization layers are studied, and microstructural and elemental analyses were performed to analyze the failure modes. The results show that the reliability of the sintered Ag joints by the traditional Ni/Ag metallization is rather limited because of poor adhesion between Ni and Ag. In contrast, the shear strength of the new Ni/Cu/Ag metallized sintered Ag joints is consistently above 40 MPa up to 500 TS cycles, with the dominant failure modes formed by Al/Ni delamination and cohesive failure. Preparing sintered Ag joints with the Ni/Cu/Ag metallization with longer sintering times removed the unwanted delamination failure mode and only left the preferred cohesive failure mode; moreover, the shear strength improved significantly, with values reaching 130 MPa. Furthermore, a new failure mode appears in the sintered Ag joint of the Ni/Cu/Ag stack, implying that the Al/Ni metallization weakness there is less of a limiting factor. This proves that our new metallization stack resolves present delamination issues in Ag sintered joints with Al heatsinks and DBA substrates and thereby supports exploiting the full potential of sintered Ag joints.