In this study, TiAlN thin film was deposited with dc magnetron sputtering on 316L stainless steel and Ti6Al4V alloy which are widely used as hip joint implants. The adhesion behaviour of TiAlN thin films was investigated by multipass scratch tester. Multipass scratching with three progressive loads was performed on each sample. Observations of the scratch tests showed that there were three main failure events which were identified and labelled as Lc1, Lc2 and Lc3. Failure mechanisms were discussed according to SEM examinations of the scratch tracks. The TiAlN films with dense and homogeneous structure preferentially grew on the plane of (200) for 316L stainless steel and (111) for Ti6Al4V alloy. During the multipass scratch test, the friction coefficients were measured between 0·02 and 0·05. The best values for the friction coefficient were obtained from the films preferentially deposited on the plane of (111). After the scratch test, the thin film was damaged by mechanisms of chipping, flaking and spalling.
Implants called miniplates, with different geometries, are used for the treatment of a fractured or diseased mandible. Generally, Ti-based miniplates in various quantities and with various geometries are fixed into the bone tissue according to the location and shape of the fracture by embedding. The aim of this study was to increase the strength of the material used in the production of miniplates by means of the equal-channel angular pressing (ECAP) treatment, and to provide a highrigidity fixation system with fewer miniplates. In this study, the ECAP method, which is one of the methods of severe plastic deformation, was applied at 4 passes at 300°C in route Bc to increase the strength of pure Ti. Then, miniplates were produced with 2 different geometries (regular and long) and 2 different properties of the Ti material (untreated and ECAP-treated). The produced miniplates were placed in the fracture line formed in the angular region of an artificial, synthetic-bone mandible. The 2-point and 3-point bending and torsion tests were conducted on these fixation systems. As a result, after the ECAP process, the yield and tensile strength of pure Ti increased by 65%, while elongation decreased by 13%. After the ECAP process, the grain size of the material was reduced from 110 μm to 200 nm. This study showed that the fixation system became more rigid due to using ECAP-treated miniplates, and this ensured lesser displacement of the fixation system.