AISI 8620 steel is used in gears and machine parts where surface wear resistance is important. The presented study focuses on different surface hardening treatments on microstructural properties and the dry sliding wear behavior of the AISI 8620 steel. The dry sliding wear test used a tribometer with constant wear test parameters according to ASTM G-99 standard. The microstructures were characterized by optical and scanning electron microscopy (SEM), energy-dispersive X-ray (EDX), and X-ray diffraction (XRD). The highest surface hardness (∼1,507 HV) occurs in the boronized sample, attributed to the hard, iron borides (FeB, Fe 2 B, Fe 3 B) layers. The minimum surface hardness (∼507 HV) is determined in nitrided samples. The maximum case hardening depth (∼0.90 mm) is obtained in nitrided samples, as the minimum value of case depth (∼0.1 mm) was found in boronized samples. The mean coefficient of friction was highest for nitrided (0.622) and lowest for boronized (0.367) samples. Boronizing also gave the minimum wear (1.705 mm 3 , 1 mg), compared with nitriding (13.5 mm 3 , 1.8 mg) and carburizing (43.57 mm 3 , 4.9 mg). The boronized samples exhibited the best wear properties. According to the optical profilometer results of worn samples; the carburized sample exhibits a broad and deep wear track (volume loss 43.57 mm 3 ), indicating severe abrasive wear due to lower surface hardness, the boronized sample showed the narrowest and shallowest wear track (volume loss 1.705 mm 3 ), because of superior wear resistance from the dense, hard iron boride layer while the nitrided sample having moderate wear depth and volume loss (13.5 mm 3 ), indicating intermediate wear resistance attributed to a thinner, harder nitride layer providing moderate protection.
Aluminum has many advantages, such as being lightweight, but it may not provide sufficient wear resistance for some applications. Tantalum oxide is a ceramic-based coating layer that can improve wear resistance. In this study, 2024 aluminum alloy samples with different surface treatments were coated with amorphous Ta2O5 using the RF spraying method under the same conditions. Polishing, 10% HCl solution, 5% NaOH solution, and 50% HNO3 solution, as well as sandblasting, were applied to the surfaces of aluminum alloys separately, and the sample groups were coated. The effects of pre-coating surface treatments on coating morphology and wear resistance were investigated. The surface morphologies of the coatings were examined using scanning electron microscopy, electron dispersion spectroscopy, and X-ray diffraction. Wear tests were then conducted to determine the mechanical properties, and after the tests, scanning electron microscopy examinations and volume loss calculations were performed using a profilometer. The wear test results were discussed and compared. The investigation yielded continuous, homogeneous, and crack-free coatings on the 2024 aluminum alloy surfaces. However, the wear resistance of these coatings was compromised by acid etching. Following polishing and sandblasting, the coated surfaces experienced a decrease in volume losses from abrasion by 4.3% and 44.8%, respectively, compared to the uncoated samples.
24 April 2024 in International Journal of Metalcasting
This study investigates the effect of two-step solution treatments and aging times on the microstructure and mechanical properties of B357 Al–Si alloy, part of the most widely used cast aluminum alloy. Three sets of artificial aging heat treatments were conducted on the tensile samples prepared from B357 alloy produced by low-pressure die casting. Firstly, the conventional artificial aging heat treatment (T6) was carried out by solutionizing the tensile samples at 543 °C for 8.5 h, water quenching at 60 °C, and then artificially aging for 8.5 h at 160 °C. In the two-step solution treatment, the samples were solutionized at 400, 440, 480, and 520 °C for 4 h and then solutionized at 543 °C for 8.5 h and water quenched to 60 °C and then artificially aged for 8.5 h at 160 °C. Thirdly, the samples were solutionized at 480 °C for 4 h, solutionized at 543 °C for 8.5 h, water quenched to 60 °C, and artificially aged for 3–192 h. Despite different solutioning and aging processes, no significant differences were observed in the microstructures of the samples. Si particle coarsening was observed with increasing solution temperature (400–520 °C) and aging times (3–192 h). Si-containing dispersoids and dispersoid-free zones (DFZ) were observed in the primary-α matrix. While DFZ width increased with temperature and aging, dispersoid zones in primary-α dendrites significantly decreased. Differential Scanning Calorimetry (DSC) analysis shows that two-step solution treatment in B357 alloy increases β′ precipitates for Mg2Si precipitation strengthening. The two-step solutionized and aged sample showed the best combination of strength and ductility among all aged samples. B357 alloy exhibited the highest yield and tensile strength (309.7, 366.1 MPa) with 6% elongation for two-step solutionizing and 48 h aging. All aged B357 alloys showed ductile fracture as the primary fracture mode. However, brittle fractured Si particles were observed on the fracture surfaces.
In this study, 1% Fe-doped ZnO thin films were deposited using Ultrasonic Spray Pyrolysis (USP) to examine their structural, morphological, and photocatalytic properties. Heat treatment was applied to 1% Fe-doped ZnO thin films produced with USP at 500 ºC for different times (1, 3, and 5 hours). The results of the samples heat-treated for different times were compared with the as-deposited sample in terms of morphological, structural properties, and photocatalytic degradation efficiency. It was observed that the ZnO thin films with a heat treatment time of 3 hours had more distinct crystal structures, and their surface morphologies were more regular and homogeneous. When the photocatalytic behaviors were examined, it was determined that the degradation efficiency of the samples heat-treated for 3 hours was better than the other samples. In conclusion, this study shows that the heat treatment time of 1% Fe-doped ZnO thin films deposited by USP significantly affects the films' structural, morphological properties, and photocatalytic activity behaviors. These results emphasize that the heat treatment time of 3 hours should be preferred and guide future research in thin film production and photocatalytic applications.