In this study, 1% Fe-doped ZnO thin films were deposited using Ultrasonic Spray Pyrolysis (USP) to examine their structural, morphological, and photocatalytic properties. Heat treatment was applied to 1% Fe-doped ZnO thin films produced with USP at 500 ºC for different times (1, 3, and 5 hours). The results of the samples heat-treated for different times were compared with the as-deposited sample in terms of morphological, structural properties, and photocatalytic degradation efficiency. It was observed that the ZnO thin films with a heat treatment time of 3 hours had more distinct crystal structures, and their surface morphologies were more regular and homogeneous. When the photocatalytic behaviors were examined, it was determined that the degradation efficiency of the samples heat-treated for 3 hours was better than the other samples. In conclusion, this study shows that the heat treatment time of 1% Fe-doped ZnO thin films deposited by USP significantly affects the films' structural, morphological properties, and photocatalytic activity behaviors. These results emphasize that the heat treatment time of 3 hours should be preferred and guide future research in thin film production and photocatalytic applications.
30 December 2022 in Gazi Üniversitesi Fen Bilimleri Dergisi Part C: Tasarım ve Teknoloji
Impact of annealing on structural, morphological, elemental, and optical properties of bilayer ZnO/Al2O3 film has been investigated. Bilayer film has been deposited on microscope slides by ultrasonic spray pyrolysis method at 350°C substrate temperature. Then, this film has been annealed at 400°C, 500°C, and 600°C under atmospheric conditions, respectively. Structural analyses have been revealed that bilayer films have polycrystalline with hexagonal wurtzite structures of ZnO. Also, there is no other structures have been found like Zn-Al etc. Morphological and elemental analyses have been presented that the alterations of surface, and diffusions of Al to ZnO layer. Cross-sectional images have been revealed the film thickness between 0,78-1.56 m. Optical method have been used for calculation of optical band gap values of the films which are found between 3.17-3.25 eV. The results revealed that annealing leads to diffusion from the bottom layer Al2O3 of the material to the upper layer, ZnO. In addition, it was determined that the as-deposited ZnO/Al2O3 film is still leading in terms of the investigated properties.
In accordance with novel strategy, the strontium hexaferrite magnet were produced by mechanochemical synthesis process using mill scale waste and strontium carbonate, and the changes in structural and magnetic properties depending on temperature were investigated to improve electrical motors. The strontium carbonate and the mill scale were prepared in a stoichiometric ratio of 1:6, and this stoichiometric mixture was subjected to a mechanochemical synthesis process for 16 hours. The synthesized powder was annealed at 850-1000°C temperatures. Increasing the SrFe12O19 phase ratio ensured the magnetic flux density to rise, and the magnetic flux density, which was 486 mT at 850°C, increased to 587 mT at 1000°C. The coercivity values of nano-sized strontium hexaferrite powders were determined as 2814, 4405, 5227, 5505, and 3415 Oe. The highest (BH)max value was calculated as 5.77 MGOe at 975°C annealing temperature. The highest Curie temperature was measured as 474°C at 975°C annealing temperature.