Surface transfer doping of diamond has been demonstrated using MoO3 as a surface electron acceptor material. Synchrotron-based high resolution photoemission spectroscopy reveals that electrons are transferred from the diamond surface to MoO3, leading to the formation of a sub-surface quasi 2-dimensional hole gas within the diamond. Ex-situ electrical characterization demonstrated an increase in hole carrier concentration from 1.00 × 1013/cm2 for the air-exposed hydrogen-terminated diamond surface to 2.16 × 1013/cm2 following MoO3 deposition. This demonstrates the potential to improve the stability and performance of hydrogen-terminated diamond electronic devices through the incorporation of high electron affinity transition metal oxides.
Homoepitaxial diamond has been used to demonstrate the RF performance of 50-nm gate length hydrogen-terminated diamond field-effect transistors. An extrinsic cutoff frequency of 53 GHz is achieved which we believe to be the highest value reported for a diamond-based transistor. The generation of an RF small signal equivalent circuit is used to extract device elements to better understand variation between intrinsic and extrinsic operation. An intrinsic cutoff frequency of 90 GHz is extracted through this process, verifying the requirement to minimize access resistance to maximize the potential high-frequency performance of this technology.
19 May 2017 in IEEE Journal of the Electron Devices Society
A method to improve thermal management of β-Ga 2 O 3 FETs is demonstrated here via simulation of epitaxial growth on a 4H-SiC substrate. Using a recently published device as a model, the reduction achieved in self-heating allows the device to be driven at higher gate voltages and increases the overall performance. For the same operating parameters an 18% increase in peak drain current and 15% reduction in lattice temperature are observed. Device dimensions may be substantially reduced without detriment to performance and normally off operation may be achieved.
We present the dc operation of hydrogen-terminated diamond field-effect transistors (FETs) with gate lengths of 1 μm to 50 nm. The 50-nm device metrics include a maximum drain current of 290 mA/mm and a peak extrinsic transconductance of 95 mS/mm. As the device gate length is reduced, peak intrinsic transconductance is increased substantially to a value of 650 mS/mm for the 50-nm device. A minimum Ion/Ioff ratio of ~ 1.5 × 104 is maintained at this reduced gate dimension. These results appear highly promising for the improvement of hydrogen-terminated diamond FET high-frequency performance through reduction of the device gate length to sub-100-nm dimensions.
20 February 2015 in IEEE Transactions on Electron Devices
Three sets of different gate-length field-effect transistors (250, 120, and 50 nm) have been defined on homoepitaxial hydrogen-terminated diamond with the 50-nm device being the smallest gate length diamond transistor fabricated to date. DC- and small-signal RF measurements were undertaken to compare the operation of these gate nodes. RF small-signal equivalent circuits were generated to contrast individual components and better understand the operation at various gate dimensions. Scaling the gate length to smaller dimensions leads to an increase in the cutoff frequency of these devices although parasitic elements are found to dominate at the shortest gate length of 50 nm, limiting the outstanding potential of these devices.