Alexander I. Burya

Alexander I. Burya

Auto-generated profile, based on publicly available information

Alexander I. Burya

Dnepropetrovsk State Agrarian University

Research Focus & Metrics

Academic Career Length

49Years (1978-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2007 in High Temperature
Verified
Journal Article
Closed access
PDF file
IDI. V. Dolbin
I. V. Dolbin
ABA. I. Burya
A. I. Burya
GKG. V. Kozlov
G. V. Kozlov
The important part played by the structure of polymer melt in determining the temperature of intensive degradation is demonstrated. This characteristic depends on the chemical structure of polymer, expressed in terms of glass transition temperature, compactness of coiled macromolecule in the melt, and type of oxidizer diffusion. The latter factor is defined by the melt structure as well.


1 August 2017 in Discover Nano
Verified
Journal Article
Open access
PDF file
AKAndriy A. Konchits
Andriy A. Konchits
BSBela D. Shanina
Bela D. Shanina
SKSerhii V. Krasnovyd
Serhii V. Krasnovyd
ABAlexander I. Burya
Alexander I. Burya
OKOlga Yu Kuznetsova
Olga Yu Kuznetsova
The evolution of paramagnetic properties of the fullerene soot (FS), fullerene black (FB), and their polymer composites Phenylon C-2/FS, FB has been studied using the electron paramagnetic resonance (EPR) method. For the first time, a drastic growth of the EPR signals in the FB, FS, and composite samples was observed under pumping out at temperatures T = 20 ÷ 300 °C, which is attributed to the interaction between carbon defects and adsorbed gas molecules, mainly oxygen. It is shown that the ensemble of paramagnetic centers in the FB, FS, and the composite is heterogeneous. This ensemble consists of three spin subsystems 1, 2, and 3 related with different structural elements. The subsystems give three corresponding contributions, L 1, L 2 and L 3, into the overall contour of the EPR signal. The most intensive and broad signal L 3 is caused by 2D electrons from the surface of carbon flakes. Theoretical calculations of the L 3 signal line shape were carried out, and the decay rate of the integral intensity has been obtained for each component L 1, L 2, and L 3 after the contact of the sample with the ambient air. The signal decay process in the bulk composite samples is much slower due to their low gas permeability at room temperature (RT).

1 December 2007 in Theoretical Foundations of Chemical Engineering
Verified
Journal Article
Closed access
PDF file
ZAZ. Kh. Afashagova
Z. Kh. Afashagova
GKG. V. Kozlov
G. V. Kozlov
ABA. I. Burya
A. I. Burya
GZG. E. Zaikov
G. E. Zaikov
It is shown that the theoretical models developed to estimate the microhardness of homogeneous solids cannot adequately describe this characteristic for particulate-filled polymer nanocomposites. This description can be accomplished in terms of the model proposed for heterophase materials, which takes into account the degree to which the polymer matrix is filled with filler nanoparticles coated by the interfacial layer.

27 March 2006 in Journal of Applied Polymer Science
Verified
Journal Article
Closed access
PDF file
GKG. V. Kozlov
G. V. Kozlov
ABA. I. Burya
A. I. Burya
IDI. V. Dolbin
I. V. Dolbin
GZG. E. Zaikov
G. E. Zaikov

13 August 2014 in Advanced Materials Research
Verified
Journal Article
Closed access
PDF file
ABAlexandr Burya
Alexandr Burya
YYYekaterina Yeriomina
Yekaterina Yeriomina
XQXiang Yang Qian
Xiang Yang Qian
XFXiang Ming Feng
Xiang Ming Feng
Introducing carbonyl nickel’s fine particles into a thermo-resistant polyamide phenylone can significantly improve thermo-physical characteristics of the CM and extend the operational temperature range of products made from these materials. Introducing carbonyl nickel in the amount of 5 – 20 mass %, thermo-resistance of phenylon C-1 increases by 10-30 degrees (most significantly in the case of a 20 % content), thermal conductivity grows by 38 %, and temperature conductivity of composite materials ranges from 1.75∙10-4 to 1.9∙10-4, which is 1.3 - 1.4 times as high as that of the initial phenylon.