The press and sinter method remains the standard among powder metallurgy processes for powdered stainless-steel materials. It delivers low cost, low oxidation rate, and adequate corrosion resistance. Furthermore, 17-4PH is a martensitic stainless-steel that is commonly used for high-strength and medium-ductility stainless steel parts. However, a few studies have investigated the press and sinter method for producing 17-4PH parts. This shortage is due to the high hardness (low compressibility) of 17-4PH powder. Thus, the main objective of this study is to evaluate the press and sinter method in terms of the manufacturing process, the influencing factors, and the theoretical basis of press and sinter methods in conjunction with metal injection molding technology for the production of 17-4PH parts. First, the literature and monographs are examined and summarized to cover the previous results, research progress, development trends, and applications of press and sinter method 17-4PH parts. Following the theoretical analysis, the practical investigation was conducted by producing parts with cold pressing from 800 to 1600 MPa, followed by sintering: the sintering temperature was 1200 °C for one hour under a protective vacuum atmosphere. ImageJ analysis was performed to measure the sinter density. The results showed an increase in relative sinter density from 84.43% to 96.43% for 800 and 1600 MPa, respectively, while the earlier results reached 93.47%. Overall, the press and sinter method enables the production of high-hardness 17-4PH parts with a high density, without using additives like lubricants, wax, or alloying elements.
Aluminium Covetic metallurgical synthesis along with the characterization of cast material results were presented in this paper. Aluminium- 3% graphite (carbon) composites were fabricated by applying different voltages and amperages of direct current through the stir-casting process. This process, called Covetic based on patent applications of Third Millennium Metals. Obtained casts were tested for their chemical composition, density, tensile strength, hardness, microstructures, and electrical conductivity measurements using an Oxford PMI-Master Pro spark emission spectrometer, a DA-300M density measurement device, a WDW-200 universal tensile test machine, a HBA-3000S automatic Brinell Hardness Tester, a scanning electron microscope with Energy-Dispersive Spectroscopy and an AT512 Precision Ohmmeter, respectively. Moreover, increasing of amperages and/or decreasing of voltages of direct current ensured considerable increasing of electrical conductivity (≈ 34%), the notable decrement in the density (≈ 0.94%), an enhancement in the tensile strength (≈ 18%) and the hardness (≈ 15%) of aluminium Covetic casts compared to the parent metal. In summary, results show that the increasing of amperages and/or decreasing of voltages of direct current has a superior influence on improving electrical conductivity of aluminium-graphite Covetic casts with better mechanical properties.
The density, compressive strength, and microstructure analyses of gas-atomised 17-4 PH samples produced by the press and sinter method (PSM) were investigated to evaluate the effects of various factors, including cold pressing, sintering time, and conventional sintering temperature. A challenge that arose from using 17-4 PH powder was that it produced PSM parts with significantly low density due to its extremely high hardness. The evaluation procedures included Archimedes' density method, regression analysis, microstructure observation analyses (optical, SEM, and EDS), X-ray diffraction, Vickers hardness measurements, and compression strength measurements. Despite employing a low sintering temperature of 1200 °C, the work highlighted that increasing the cold pressing and sintering time aimed to improve the sinter density to approximately 98 %. A linear regression model aligned with the actual results concerning the effect of sintering time on relative sinter density, while a polynomial regression model was developed to describe the relationship between sintering temperature and relative sinter density. Compared with the reported literature, this work achieved improvements in relative sinter density (5 %), Vickers hardness (40 %), and compressive yield strength (10 %), respectively. The low sintering temperature minimised volume shrinkage. The 7 h of sintering resulted in smoother grain boundaries compared to those of 2 h. Future research can utilise the extensive investigation data to develop a mathematical model for predicting the density of PSM 17-4 PH materials.