Bryan Bilyeu

Bryan Bilyeu

Auto-generated profile, based on publicly available information

Bryan Bilyeu

Department of Chemistry, Xavier University of Louisiana, 1 Drexel Drive, New Orleans, LA 70125, USA

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 July 2013 in Chemical Engineering Journal
Verified
Journal Article
Closed access
JCJulian Cruz-Olivares
Julian Cruz-Olivares
CPCésar Pérez-Alonso
César Pérez-Alonso
CBCarlos Barrera-Díaz
Carlos Barrera-Díaz
FUFernando Ureña-Nuñez
Fernando Ureña-Nuñez
MCM.C. Chaparro-Mercado
M.C. Chaparro-Mercado
BBBryan Bilyeu
Bryan Bilyeu

15 July 2019 in Heliyon
Verified
Journal Article
Open access
CLCristina A. De León-Condés
Cristina A. De León-Condés
GRGabriela Roa-Morales
Gabriela Roa-Morales
GMGonzalo Martinez-Barrera
Gonzalo Martinez-Barrera
CCCarmina Menchaca Campos
Carmina Menchaca Campos
BBBryan Bilyeu
Bryan Bilyeu
HTHelen Paola Toledo-Jaldin
Helen Paola Toledo-Jaldin
In this work, waste expanded polystyrene (WEPS) was irradiated with gamma rays, ranging doses from 100 kGy to 1,000 kGy. After irradiation, the WEPS had decrease on its glass transition temperature (Tg), as consequence of the scissions of its polymer chains. Then, the irradiated WEPS was sulfonated, and its degree of sulfonation (DS) was measured. The highest DS value, 46.6%, was obtained for an irradiation dose of 200 kGy. The sulfonated and irradiated polystyrene (denominated as iS-WEPS), was used as a support of iron oxide nanoparticles. Such composite system was denominated (FeO-NPs + iS-WEPS). The results show nanoparticle sizes of 31.5 nm containing 21.97% iron oxide. The composites followed a pseudo-second order model, with a maximum adsorption capacity of 20 mg/g, and an equilibrium time of 30 min, according to the Langmuir model. Moreover, the optimal conditions followed by the Fenton process were: pH = 3.2, H2O2 concentration = 0.32 mM/L, composite concentration (FeO-NPs + iS-WEPS) = 2 g/L, and a reaction time 20 min. Finally, 99% removal of indigo carmine dye was achieved, and a reduction of 83% of COD in textile wastewater.

1 July 2021 in Desalination and Water Treatment
Verified
Journal Article
Open access
CLCristina A. De León-Condés
Cristina A. De León-Condés
GRGabriela Roa-Morales
Gabriela Roa-Morales
GMGonzalo Martinez-Barrera
Gonzalo Martinez-Barrera
PHPatricia Balderas Hernández
Patricia Balderas Hernández
BBBryan Bilyeu
Bryan Bilyeu