21 March 2023 in Journal of Applied Physics
Cryogenic etching of a-Si, SiO2, and Si3N4 materials by CHF3/Ar inductively coupled plasma is investigated in a range of temperature from −140 to +20 °C. Samples of the three different materials are placed together on the same silicon carrier wafer. Depending on the experimental conditions, etching or deposition regimes were obtained on the samples. The thickness variation was measured by spectroscopic ellipsometry. A process window between −120 and −80 °C was found in which the Si3N4 surface is etched while CFx deposition is obtained on a-Si and SiO2 surfaces, resulting in the infinite etching selectivity of Si3N4 to the other materials. At high enough self-bias (−120 V) and very low temperature (<−130 °C), Si3N4 etch is reduced down to a very low value, while a-Si and SiO2 are still being etched, which inverses the selectivity between Si3N4 and the two other materials. EDX analyses of a Si3N4/a-Si/SiO2 layer stack after the same etching process carried out at 20 and −100 °C confirm the presence of carbon and fluorine on a-Si at low temperature, showing the effect of the low temperature to switch from the etching to deposition regime on this material.
20 January 2025 in Applied Physics Letters
Ultraviolet (UV) absorption spectroscopy is used to monitor the CF radical density in CF4 inductively coupled plasma (ICP) plasmas as a function of the substrate temperature. The CF density decreases dramatically when the wafer temperature is reduced from 20 to −130 °C by applying identical plasma conditions, demonstrating that the CF surface sticking coefficient increases as the surface temperature is reduced. This suggests that CF4 plasma could be used to form sidewall passivation layers and perform anisotropic etching at cryogenic temperature, which is impossible at room temperature. Subsequently, a cyclical Bosch type etching process of silicon was evaluated at −100 °C using CF4 plasma to passivate the trench sidewalls. Anisotropic etch profiles were obtained with an etch rate of 4.4 μm/min. Compared to a typical Bosch process using highly polymerizing c-C4F8 plasma, chamber wall contamination could be significantly reduced, alleviating a major issue of this cyclic process. Furthermore, CF4 has a 28% lower global warming potential than c-C4F8.
1 January 1999 in High Temperature Material Processes: An International Quarterly of High-Technology Plasma Processes
One of the main challenges of modern plasma chemistry is to develop a powerful and high pressure discharge generating a non equilibrium cold plasma for chemical applications. Intermediate discharges between hot quasi equilibrium plasma and cold non equilibrium plasma are subjected to a new interest. For various applications, the behaviour of the discharge is determined mainly by processes of high temperature column of plasma interaction with cold gas flow. It means that hydrodynamic processes play a significant role and strong interaction of high temperature discharge with cold gas flow must be taken into account. In order to study such an interaction we performed experiments in which anode and cathode spots remained fixed at the tips of electrodes. In these conditions it is very easy to determine the characteristics of the discharge motion. One of most important experimental result is the so called : back-breakdown phenomenon. Then it is possible to express the motion of the discharge as a function physical parameters of the ionised gas. A simple model of interaction is introduced which allows a better understanding of various chemical reactors.
23 September 2024 in Journal of Micromechanics and Microengineering
The Bosch process was studied at a substrate temperature of −100 °C and compared to etchings performed at room temperature, as in the general case. The tests were realized using an inductively coupled plasma reactor by varying C4F8 passivating gas flow injections both at +20 °C and −100 °C. It was observed that the Bosch process is effectively temperature dependent and that the necessary C4F8 passivating gas flow can be reduced to obtain similar anisotropic profiles at −100 °C compared to the ambient temperature process. For example, in one of the studied cases, a fluorocarbon injection of 8 sccm was sufficient to obtain an anisotropic etch rate of up to 4.4 μm min−1 at −100 °C whereas the profile obtained at +20 °C using the same parameters presents lateral etching defects with a reduced etch rate of 2.4 μm min−1. At this point, the C4F8 flow must be increased to 12 sccm (50% more) to retrieve an anisotropic profile with an etch rate of 4.0 μm min−1. In the case of cryogenic Bosch (cryo-Bosch) processing, C4F8 feed dosing has a greater influence on the passivation regime which affects the subsequent etching result but it can be easily refined through the optimization of process parameters. An in-situ ellipsometry study of the deposition rate of C4F8 on both polycrystalline silicon (p-Si) and SiO2 substrates was realized by varying the gas flow at −100 °C and +20 °C. This study shows that the deposited fluorocarbon material is approximately a hundred times thicker at cryogenic temperatures using the same process parameters. Scanning electron microscopy (SEM) observation of these samples are in adequacy with the ellipsometry results. Cryo–Bosch etching also results in a slightly higher etch rate compared to room temperature processing when analyzing similar anisotropic profiles. Si:SiO2 etching selectivity is significantly increased at −100 °C although the aspect-ratio dependent etching phenomenon is more important.
17 April 2023 in Journal of Vacuum Science & Technology A
Atomic layer etching (ALE) of GaN on silicon substrates has been investigated using fluorine-based chemistry. The ALE process used for this study consists of a modification step using SF6 plasma and a removal step using argon plasma. Two configurations were studied in which the distance between the sample and the plasma source was modified. The energy scan, synergy, selective etching of GaFx by Ar+ ion bombardment, and self-limiting etching regime of the ALE of GaN were first investigated. An etch per cycle of 0.50 nm/cycle averaged over 100 cycles was reached for GaN ALE. The self-limiting regime was also obtained for both SF6 and argon plasma steps. Moreover, a synergy rate as high as 78% was achieved. It was found that the GaFx-modified layer can be selectively sputtered by applying a self-bias voltage while the argon ion energy is maintained below the sputtering threshold of GaN.
26 June 2009 in Semiconductor Science and Technology