In order to explore the influence of rare earth element Y on the electrical contact properties of Pt–Ir alloys, Pt–10Ir–Y and Pt–25Ir–Y were prepared via arc melting combined with thermal processing, and electrical contact experiments were carried out with a DC voltage of 24 V and current ranging from 5 A to 25 A. Comparative analyses were conducted to analyze the changes in the break arc duration and arc energy, as well as the contact resistance before and after the addition of Y. The arc erosion surface morphology was characterized, and the transfer behavior of the alloys was discussed. The results show that at 5 A and 25 A, adding Y improves the stability of the arc duration of the Pt–Ir alloy, but it increases the overall arcing energy and decreases the stability. The contact resistance of the Pt–Ir alloy shows a clear partitioning phenomenon; the partitioning phenomenon disappears after the addition of Y, and the contact resistance fluctuates around the average value. The material transfer direction of the Pt–Ir alloy is affected by the current change, while the material transfer direction of the Pt–Ir–Y alloy is always from cathode to anode. The research results provide a reference for the performance optimization of Pt–Ir alloys.
The Pt–Ir alloy is an important electrical contact material in the aerospace field, and its electrical contact performance directly affects the reliability and stability of the circuit system. In order to elucidate the effect of Y on the breaking arc behavior of Pt–Ir alloys at different voltages, Pt-10Ir-1Y and Pt-25Ir-1Y alloys were prepared using melting and thermal processing, and the electrical contact tests were carried out at DC 15 A 12 V, 24 V, and 36 V. When comparing the results of Pt-10Ir and Pt-25Ir electrical contact tests, they showed that Y doping provided a tendency to concentrate individual arc erosion regions. Meanwhile, the comparative study showed that the addition of Y could inhibit the tendency of the Pt–Ir arc time to increase with voltage. At 36 V, the overall arc time of Pt–Ir–Y was significantly lower than that of Pt–Ir, and the fluctuation in arc time and arc energy was reduced. In addition, Y reduced the welding force of Pt–Ir alloys at 12 V, while Y improved the stability of the welding force of Pt–Ir alloys at 24 V. It could be seen that Y was favorable to improving the arc erosion resistance of the Pt–Ir alloy under certain conditions. The contact resistance analysis showed that there was an obvious partitioning phenomenon in the contact resistance of Pt–Ir alloys, and Y changed in this phenomenon at a certain voltage range. In addition, the material transfer direction of the Pt–Ir alloy was from the anode to the cathode, which was not affected by the voltage change, while the addition of Y changed the material transfer direction from the cathode to the anode, which was likely caused by the change from the metal-phase arc dominance to gas-phase arc dominance.
The first-step drawing process of the platinum-clad nickel composite bar was numerically simulated using DEFORM 3D finite element analysis software. The Taguchi method was used to study the effect of the first-step drawing parameters (the semi-angle of die α, the friction coefficient between the platinum tube and die μ1, the friction coefficient between the platinum tube and nickel rod μ2 and the outer diameter of the original platinum tube D) on the effective stress of platinum-clad nickel bar. Then, the optimal combination of parameters (D = 7.55 mm, μ1 = 0.2, μ2 = 0.3, α = 3°) was obtained. Furthermore, the results of the deformation behavior, cladding behavior, stress effectiveness and the distribution of the damage of the composite bar using optimization schemes were compared and analyzed with Numerical Simulations 8, which showed the worst result. Meanwhile, the experimental results were in general agreement with the simulation results of optimal combination of parameters, indicating that our simulation results are plausible. This has certain guidance significance to improve the quality of platinum-clad nickel composite wires in actual production.
Platinum-clad nickel composite wires with platinum layer thicknesses of 5 μm and 8 μm were prepared by a cladding drawing process. Oxidation experiments were performed using a muffle furnace at temperatures of 500 °C, 600 °C, 700 °C, and 800 °C for 1 h, 2 h, and 3 h. The oxidized samples were examined for high-temperature oxidation behavior using scanning electron microscopy (SEM) with an energy-dispersive X-ray (EDX) spectrometer attached. The results showed that the interface bond between the platinum cladding and the nickel core wire was serrated and that the thickness of the platinum cladding was not uniform. At low temperatures (500 °C and 600 °C), the diffusion rate of the nickel was low. The composite wire could be used for a short time below 600 °C. When the temperature reached 700 °C and above, the nickel diffused to the surface of the composite wire and was selectively oxidized to form a nickel oxide layer. The research results provide a theoretical reference for the selection of a service temperature for platinum-clad nickel composite wires used as the lead material for thin-film platinum resistance temperature sensors.