Thermal-cyclic atomic layer etching of a Co film and a fine pattern with a smooth etched surface by plasma oxidation and organometallization is demonstrated. One cycle of the etching process consists of a two-temperature process. In the first step, plasma oxidation of Co is carried out at a low temperature of 25 °C to obtain a smooth Co oxide layer. In the second step, the Co oxide is organometallized with acetylacetone and desorbs at a high temperature of 210 °C that is suitable for organometallization and desorption. The etched amount per cycle is 0.6 nm, which is the same as the saturation amount of oxidation. A smooth etched surface is obtained after 20 cycles with a root mean square roughness of 0.53 nm, which is only slightly higher than the initial value of 0.34 nm. High etching selectivity over barrier metal of titanium-nitride was obtained. The two-step temperature cycle is crucial to achieve favorable etching with smooth etched surfaces.
1 December 2007 in IEEE Transactions on Ultrasonics, Ferroelectrics, and Frequency Control
Characteristics of metal-ferroelectrics-metal (MFM) capacitors and metal-ferroelectrics-insulator-semi-conductor (MFIS) diodes with poly(vinylidene fluoride-trifiuoroethylene) [P(VDF-TrFE)] copolymer films thinner than 100 nm were investigated. The films were prepared by spin-cast process and were annealed at 140degC in air for crystallization. The ferroelectric properties are equivalent to those of oxide ferroelectrics, even under low voltage or high frequency operation.
Thermal-cyclic atomic layer etching of Co blanket film and a fine pattern by plasma oxidation and organometallization were investigated. To obtain a smoothly etched surface and self-limiting etching, a two-step temperature-etching process was used. Co was first oxidized using O2 plasma at a low temperature of 25 °C. Then, the Co oxide formed in the first step was organometallized with acetylacetone (acacH) and sublimed at a high temperature of 210 °C, which is appropriate for organometallization and sublimation. The etched amount per cycle was 0.6 nm. This value is the same as the saturated oxidation amount. The root-mean-square roughness after 20-cycle etching was 0.53 nm, and an atomically smooth etched surface was obtained. From the x-ray photoelectron spectroscopy (XPS) analysis, the oxidation state of Co oxide with a 530-eV O1s peak was dominant for organometallization with acacH. As the temperature increased, the O1s XPS peak of the Co oxide shifted lower to 529 eV and formed a columnar-shaped oxide. However, with acacH, oxide was organometallized when the O1s peak was at 530 eV.