In the past, studies have been performed to follow chain dynamics in an equilibrium polymer melt using low molar mass polymers. Here we show that in linear ultrahigh molecular weight polyethylene entanglements formed during or after polymerization are influencing differently the overall chain topology of the polymer melt. When a disentangled UHMWPE sample is crystallized under isothermal conditions after melting, two endothermic peaks are observed. The high temperature peak is related to the melting of crystals obtained on crystallization from the disentangled domains of the heterogeneous (nonequilibrium) polymer melt, whereas the low melting temperature peak is related to the melting of crystals formed from entangled domains of the melt. On increasing the annealing time in melt, the enthalpy of the lower melting temperature peak increases at the expense of the high melting temperature peak due to the transformation of the disentangled nonequilibrium melt into the entangled equilibrium one. However, independent of the equilibrium or nonequilibrium melt state, the high melting temperature peak is observed when the disentangled samples are left to isothermally crystallize at a specific temperature, although with a decrease in bulk crystallinity. A commercial (entangled) sample, instead, shows both shift in the position of the melting temperature peak and drop in crystallinity. To ascertain that entanglements are the cause for the observed difference, experiments are performed in the presence of reduced graphene oxide (rGON): the melting response of disentangled UHMWPE crystallized from its heterogeneous melt state remains nearly independent of the annealing time in melt. This observation strengthens the concept that in the presence of a suitable filler, chain dynamics is arrested to an extent that the nonequilibrium melt state having lower entanglement density is retained.
Various oxirane monomers including alkyl ether or allyl-substituted ones such as 1-butene oxide, 1-hexene oxide, 1-octene oxide, butyl glycidyl ether, allyl glycidyl ether, and 2-ethylhexyl glycidyl ether were anionically copolymerized with CO2 into polycarbonates using onium salts as initiator in the presence of triethylborane. All copolymerizations exhibited a “living” character, and the monomer consumption was monitored by in situ Fourier-transform infrared spectroscopy. The various polycarbonate samples obtained were characterized by 1H NMR, GPC, and differential scanning calorimetry. In a second step, all-polycarbonate triblock copolymers demonstrating elastomeric behavior were obtained in one pot by sequential copolymerization of CO2 with two different epoxides, using a difunctional initiator. 1-Octene oxide was first copolymerized with CO2 to form the central soft poly(octene carbonate) block which was flanked by two external rigid poly(cyclohexene carbonate) blocks obtained through subsequent copolymerization of cyclohexene oxide with CO2. Upon varying the ratio of 1-octene oxide to cyclohexene oxide and their respective ratios to the initiator, three all-polycarbonate triblock samples were prepared with molar masses of about 350 kg/mol and 22, 26, and 29 mol % hard block content, respectively. The resulting triblock copolymers were analyzed using 1H NMR, GPC, thermogravimetric analysis, differential scanning calorimetry, and atomic force microscopy. All three samples demonstrated typical elastomeric behavior characterized by a high elongation at break and ultimate tensile strength in the same range as those of other natural and synthetic rubbers, in particular those used in applications such as tissue engineering.
Reprocessing of reinforced composites is generally accompanied by loss of value and performance, as normally the reinforcing phase is damaged, or the matrix is lost in the process. In the search for more sustainable recyclable composite materials, we identify blends based on poly(L-lactide) (PLA) and thermotropic liquid crystalline polymers (LCP) as highly promising self-reinforced thermoplastic composites that can be recycled several times without loss in mechanical properties. For example, irrespective of the thermal history of the blend, injection molded bars of PLA containing 30 wt% LCP exhibit a tensile modulus of 6.4 GPa and tensile strength around 110 MPa, as long as the PLA matrix has a molecular weight of 170 kg mol-1 or higher. However, after several mechanical reprocessing steps, with the gradual decrease in molecular weight of the PLA matrix, deterioration of the mechanical performance is observed. The origin of this behavior is found in the increasing LCP to PLA viscosity ratio: At a viscosity ratio below unity, the dispersed LCP droplets are effectively deformed into the desired fibrillar morphology during injection molding. However, deformation of LCP droplets becomes increasingly challenging when the viscosity exceeds unity (i.e. when the PLA matrix viscosity decreases during consecutive reprocessing), eventually resulting in a nodular morphology, a poor molecular orientation of the LCP phase, and deterioration of the mechanical performance. This molecular weight dependency effectively places a limit on the maximum number of mechanical reprocessing steps before chemical upgrading of the PLA phase is required. Therefore, a feasible route to maintain or enhance the mechanical properties of the blend, independent of the number of reprocessing cycles is proposed.