Previously, an innovative way to reduce rear interface recombination in Cu(In,Ga)(S,Se) 2 (CIGSSe) solar cells has been successfully developed. In this work, this concept is established in Cu 2 (Zn,Sn)(S,Se) 4 (CZTSSe) cells to demonstrate its potential for other thin-film technologies. Therefore, ultrathin CZTS cells with an Al 2 O 3 rear surface passivation layer having nanosized point openings are fabricated. The results indicate that introducing such a passivation layer can have a positive impact on open-circuit voltage (V OC ; +17%rel.), short-circuit current (JSC ; +5%rel.), and fill factor (FF; +9%rel.), compared with corresponding unpassivated cells. Hence, a promising efficiency improvement of 32%rel. is obtained for the rear passivated cells.
We report on the physical, electrical, and optical properties of Cu2ZnSnSe4 (CZTSe) solar cells based on an absorber layer fabricated by selenization of sputtered Cu, Zn, Sn multilayers. It is shown that the doping density as measured by drive level capacitance profiling is correlated exponentially to the Zn/Sn ratio of the CZTSe absorber as measured by energy dispersive X-ray spectroscopy. Furthermore, it is shown that the open circuit voltage of the cells, minority carrier lifetime, and peak position of the photoluminescence response of the absorber all correlate with the doping level and, therefore, with the Zn/Sn ratio measured in the absorber.
B-type Cu2ZnSnS4 (CZTS) thin films with varying degrees of cation order were produced and examined with resonant Raman spectroscopy. Simulations based on Vineyard's theory of order allowed kinetic analysis of the final degree of order after the applied thermal treatments. Combining the results from the simulations and the resonant Raman spectra, the kinetic parameters within the Vineyard model for the order-disorder transition in B-type CZTS were determined, as well as a method which allows quantification of the degree of order based on resonant Raman spectra. The knowledge gained about the order-disorder transition in B-type CZTS allowed the prediction of a best practice thermal treatment for high ordering. This further leads to awareness about practical limits of thermal treatments regarding the cation ordering in B-type CZTS, and suggests that such treatments are not able to produce the high cation order necessary to sufficiently reduce detrimental potential fluctuations.
Photoluminescence (PL) is commonly used for investigations of Cu2ZnSnS(e)4 [CZTS(e)] and Cu(In,Ga)Se2 (CIGS) thin film solar cells. The influence of interference effects on these measurements is, however, largely overlooked in the community. Here, it is demonstrated that PL spectra of typical CZTS absorbers on Mo/glass substrates can be heavily distorted by interference effects. One reason for the pronounced interference in CZTS is the low reabsorption of the PL emission that typically occurs below the band gap. A similar situation occurs in band gap graded CIGS where the PL emission originates predominantly from the band gap minimum located at the notch region. Based on an optical model for interference effects of PL emitted from a thin film, several approaches to reduce the fringing are identified and tested experimentally. These approaches include the use of measured reflectance data, a calculated interference function, use of high angles of incidence during PL measurements as well as the measurement of polarized light near the Brewster angle.
Kesterite Cu2ZnSnS4 (CZTS), having only earth-abundant elements, is a promising solar cell material. Nevertheless, the impact of the SnS secondary phase, which often forms alongside CZTS synthesis at high annealing temperature, on CZTS solar cells is poorly studied. We confirm, by means of X-ray diffraction, Raman scattering, and energy dispersive X-ray spectroscopy mapping, that this phase tends to segregate at both the surface and the back side of annealed CZTS films with Cu-poor and Zn-rich composition. Using electron beam-induced current measurements, it is further demonstrated that the formation of SnS on the CZTS surface is harmful for solar cells, whereas the SnS phase can be beneficial for solar cells when it segregates on the CZTS rear. This positive contribution of SnS could stem from a passivation effect at the CZTS/SnS rear interface. This work opens new possibilities for an alternative interface development for kesterite-based photovoltaic technology.