A new phosphonate modified silica (PMS) has been investigated for adsorption of Co(II), Ni(II), Cu(II), and Zn(II) in aqueous solution. The adsorbent was modified of silica by immobilizing aminoethyl dihydrogen phosphate (AEPH2) on 1,4-dibromobutane grafted silica. The physicochemical of the adsorbent was investigated using Fourier Transform Infra-red (FTIR) spectroscopy, X-ray Fluorescence (XRF), and N2 gas adsorption/desorption. The adsorption study was carried out in a batch system by mixing solution of metal ions at various pHs, contact times, and initial metal ion concentrations. The unadsorbed metals were determined by Flame Atomic Absorption Spectrophotometry (FAAS). Result of characterization showed that PMS has been successfully prepared. The product contained 45.99% (w/w) silica and 1.33% (w/w) phosphorous with surface area, pore volume, and pore size of 115.3 m2g-1; 0.7578 mLg-1; and 131.44 Å, respectively. Adsorption of metal ions on PMS occurred quite fast, less than 30 min. Modification of phosphonate on silica increased the adsorption capability, up to 8 times higher than that of unmodified silica, depending on metal ion type and pH solution. The capacity order of the metals adsorption was Cu(II)>Co(II)>Ni(II)>Zn(II). Based on the adsorption characteristic, the adsorbent is promising to be applied as a material for solid phase extraction of transition metal ions.
The effect of macrocycle ring size on the corrosion inhibition efficiency of dibenzo-12-crown-4 (DB12C4), dibenzo-15-crown-5 (DB15C5), dibenzo-18-crown-6 (DB18C6), dibenzo-21-crown-7 (DB21C7) and dibenzo-24-crown-8 (DB24C8)have been elucidated by mean of density functional calculation at B3LYP/6-31G(d) level of theory in the gas and aqueous environment. The quantum chemical parameters including the frontier orbital energies (EHOMO, ELUMO), ionization potential (I), electron affinity (A), the absolute electronegativity (χ), hardness (η), softness (σ), and the fraction of electron transferred (ΔN) are positively correlated to the corrosion inhibition efficiency (IE%) of the studied crown ethers. The calculation results indicate that DB24C8 exhibits the highest corrosion inhibition efficiency, whereas DB12C4 exhibits the lowest corrosion inhibition efficiency. The results of this study will contribute to design crown ethers potential as corrosion inhibitors.
In this research, mercapto-silica coated magnetite (Fe3O4-SiO2-SH) has been prepared in aqueous solution through a simple approach so called a one-pot process. The Fe3O4-SiO2-SH was prepared in nitrogen condition by mixing magnetite, 3-mercaptopropyltrimethoxysilane (MPTMS), and sodium silicate (Na2SiO3) solution extracted from rice hull ash, and adjusting the pH of 7.0 using hydrochloric acid. The residue was washed with deionized water, dried at 150°C and separated with an external magnetic field. In that work, the volume of MPTMS and Na2SiO3 was varied and the total amount of Si represented as silica was kept constant. Characters of the material including the functional group presence, the structure, the porosity, the morphology and stability toward various solvents were identified and evaluated. Results of characterization indicated that mercapto-silica has been coated magnetite particle with a simple one-pot process. Coating mercapto-silica on magnetite increases particle size, surface area, and chemical stability. Additionally, Fe3O4-SiO2-SH also shows high stability toward various organic solvents. The magnetic property of magnetite does not change after coating and the addition of nonmagnetic material still gives high value of maximum saturation magnetization. The presence of mercapto groups effective for interaction with heavy metal ions, the high chemical stability without removing the magnetic property promises the prospective application of Fe3O4-SiO2-SH in the future such as for separation and removal of heavy metal ions from aquatic environments.
Modification of silica coated on magnetic material iron sand with chitosan for adsorption of Au(III) has been carried out. Magnetic material (MM) from iron sand was separated using an external magnet, washed with water and HF solution 10%. MM–silica–chitosan material (MMSC) was synthesized via sol gel process and the product was characterized with Fourier Transform Infrared (FT-IR) spectrophotometer, X–ray diffractometer, scanning electron microscopy and energy dispersive X–ray, thermogravimetric analysis, and vibration sample magnetometer. Additionally, the effect of pH on the stability of MMSC has also been tested. The adsorption of Au(III) on MMSC was proceeded in a batch system with variation of pH, contact time, and concentration of absorbate. Adsorbent was separated using external magnet and concentration of Au(III) not adsorbed was analyzed using Atomic Absorption Spectrometer. Characterization result indicated that MMSC was successfully synthesized. Adsorption of Au(III) on MMSC followed pseudo second-order kinetic model with the value of adsorption rate constant (k) of 4.10 x 10-3 g mg-1 min-1 and adsorption isotherm fixed with Langmuir model with the adsorption capacity (qmax) of 149.25 mg g-1.