In this study, the effect of pure Ni and Ni–SiO2 nanocomposites coatings on corrosion, wear resistance and thermal conductivity of 316 stainless steel substrates was investigated with the purpose of extending the service life of 316 stainless steel plate heat exchangers. The nanocomposite coatings were developed by electroplating process in a Watts bath in different concentration values of SiO2 nanoparticles (10, 20 and 30 g l−1). Electrochemical corrosion was run to examine the corrosive performance of the coatings. The results showed that the Ni–SiO2 nanocomposite with concentration of 30 g l−1 had a higher corrosion resistance. A pin on disk wear test demonstrated that, in comparison to 316 stainless steel, the wear resistance of the Ni–SiO2 nanocomposite (30 g l−1) was up to 25% lower while its friction coefficient was almost the same. In addition, as measured via the laser flash method and differential scanning calorimetry, the thermal diffusivity and specific heat capacity of the sample respectively were found to be 32 and 43% lower in comparison to 316 stainless steel. Microhardness measurement via a Vickers microindenter showed that the microhardness of the Ni–SiO2 nanocomposite coating was more than three times higher than that of 316 stainless steel for all the reinforcement concentrations.
29 August 2022 in Journal of Materials Engineering and Performance
In this investigation, hybrid aluminum matrix composites reinforced with Fe-based metallic glass (FMG) and SiC particles were synthesized using spark plasma sintering (SPS) at different sintering temperatures. The effects of sintering temperature on densification, phases, microstructure, and mechanical properties of the composites were evaluated. The findings indicate that the density of the sintered samples improved with increasing the sintering temperature. The X-ray diffraction results showed no remarkable difference in the phases of the samples sintered at different temperatures; only some small structural changes occurred in the metallic glass reinforcements. The sintering temperature had a significant effect on mechanical properties. For example, the hybrid aluminum matrix composite reinforced with 3 vol% FMG and 7 vol% SiC sintered at 550°C exhibited the ultimate compressive strength of 494 MPa, which is about 47% higher than the same composite sintered at 450°C.