31 January 2021 in İstanbul Tıp Fakültesi Dergisi
İstanbul Üniversitesi Yayın Projesi
6 February 2023 in Journal of Prosthodontics
17 November 2022 in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
This study evaluates the durability of repair microshear bond strength (µSBS) of nanohybrid composite resins which surfaces are treated with different laser parameters and bur. A total of 240 nanohybrid composite resin disk shaped specimens were prepared. Then, specimens were divided into eight test groups as regards to surface treatment types (Erbium (Er:YAG) laser with seven different parameters and bur). Half of the specimens in each group were subjected to 5000 thermal cycling (TC) and the other half to 20,000 TC. Universal testing machine was used for µSBS test. The data were analyzed with a two-way analysis of variance and Tukey test. Among the specimens treated with ER:YAG laser+5000 TC, we detected the highest mean µSBS test values in the subgroups L200 and L250. Among the specimens treated with ER:YAG laser+20,000 TC, the highest mean µSBS test values were seen in the L200 subgroup. The µSBS values after the 20,000 TC were significantly lower than those after 5000 TC for all different treatment types. Thermal cycling and laser energy levels have effects on repair µSBS. Considering the bond strength and durability it seems more effective to use Er:YAG laser at 200 mJ. To repair an aged nanohybrid composite resin, Er:YAG laser surface treatments may provide some benefits by acquiring a reliable bond strength with durability. This study may give information on which parameters are more suitable to use Er:YAG laser for the repair of nanohybrid composite resins.
12 May 2023 in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
The objective of this in vitro study was to investigate the micro shear bond strength (µSBS) of mineral trioxide aggregate to four different restorative materials. Sixty mineral trioxide aggregate (MTA) samples were randomly assigned into four experimental groups based on the restorative materials used: nanohybrid resin composite as a control, giomer, alkasite and ormocer. µSBS samples were prepared for each group ( n = 15). These samples were then submitted to a µSBS test (crosshead speed, 0.5 mm/min). The resulting data were statistically analyzed by one-way analysis of variance (ANOVA), Levene, and Bonferroni tests (α = 0.05). The bond strength of the alkasite group was statistically significantly higher than all the tested groups ( p 0.05). Within the limitations of this study, alkasite restorative material could be a promising material when placed over MTA.
2 February 2023 in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
This study evaluates how pre-treatment with an MDP-containing cleaning agent (Katana Cleaner, Kuraray) influences the micro-shear bond strength (µSBS) of saliva-contaminated zirconia when used with universal adhesive (UA) systems. Rectangular specimens (2 mm × 12 mm × 15 mm) were obtained (IPS, e.max ZirCAD, MO, B65L17, Ivoclar Vivadent) and divided into three groups; a non-contaminated group (control group)(CON), a contaminated and cleaned with isopropyl alcohol group(ISP), and lastly, a group contaminated and cleaned with an MDP-containing cleaning agent(KAC). Each group was then subdivided into three subgroups according to the UAs used ( n = 12). Composite cylinders were prepared and bonded to each surface with Panavia V5 (Kuraray, Noritake Dental). A µSBS test was performed and the data were evaluated with the two-way analysis of variance (two-way ANOVA) and multiple comparisons test (α = 0.05). The highest µSBS values were obtained in the non-contaminated group ( p < 0.001), regardless of UAs. All subgroups showed lower µSBS values after saliva contamination, but KAC resulted in significantly higher µSBS values than 99% isopropanol ( p < 0.001). Overall, the lowest µSBS value was obtained with 99% isopropanol. The KAC-Clearfil UA subgroup resulted in statistically significantly higher µSBS values than the other UAs ( p = 0.035 and 0.007), although all three UAs resulted in sufficient µSBS values. This study revealed that applying KAC followed by a UA containing phosphate monomers produces promising results for improving µSBS values of zirconia, greater than results using 99% isopropanol. Clinical relevance: An MDP-containing cleaning agent followed by a phosphate monomer containing a universal adhesive is a promising method to obtain acceptable bonds with saliva-contaminated zirconia ceramics.
30 March 2022 in Meandros Medical and Dental Journal