First-principles calculation was used to systematically investigate hydrogen solubility in Pd3Ag phases. It was found that the solubility of hydrogen in Pd3Ag phases was much greater than in face-centered cubic (FCC) Pd, suggesting that Ag atoms enhanced hydrogen solubility with respect to FCC Pd. In addition, the present calculation also revealed that the anti-site defect formation enthalpies of Pd3Ag were close to zero, and the values of vacancy were positive and large, which indicated that Pd3Ag distributed compactly. In the process of hydrogen separation, anti-site defects decreased the hydrogen solubility in the Pd3Ag phases, i.e., the ordered Pd3Ag phases bestowed excellent properties of H selectivity. The results presented not only explore the fundamental properties of Pd3Ag phases and their various potential applications, but also agree with experimental observations reported in the literature.
8 January 2020 in Journal of Physics: Condensed Matter
Interface adhesion and stability between titanium and carbon materials have been investigated by first-principles calculation, in which three different DFT-PBE, DFT-LDA and optB88-vdW approaches are considered. Our calculation reveals that the formation of carbon vacancy in graphene would enhance the interface stability and increase interfacial strength, which may be due to a strong hybridization between titanium atom and the sp 2 dangling bonds of the carbons near the vacancy. It is also found that the van der Waals interaction has less effects on cohesion properties of the titanium/graphite interfaces, and the Ti-C bond of titanium–carbon interfaces is weaker than that of the TiC bulk. The derived results are discussed in depth by means of electron distribution and Bader transfer analysis, and could be used as a guiding parameter for exploring the fundamental properties of titanium–carbon products as well as various potential applications.
1 December 2011 in Computational and Theoretical Chemistry