This paper reports a study on the effect of Al2O3 nanoparticles on the adhesion strength of steel-glass/epoxy composite joints bonded by a two-component structural acrylic adhesive. The addition of Al2O3 nanoparticles to the two-component acrylic adhesive led to a remarkable enhancement in the shear and tensile strength of the composite joints. The shear and tensile strength of the adhesive joints increased by addition of Al2O3 up to 1.5 wt%, which decreased by further addition of the nanofiller. Introduction of the nanoparticles caused a reduction in the peel strength of the joints. DSC analysis revealed that the glass transition temperature (Tg) of the adhesives rose by increasing the nanofiller content. The advancing water contact angle was decreased for adhesives containing nanoparticles. SEM micrographs indicated good dispersions of the Al2O3 nanoparticles within the acrylic matrix in the specimens with up to 1.5 wt% Al2O3 and revealed that addition of nanoparticles altered the fracture morphology from smooth to rough fracture surfaces.
This article reports a study on the effect of TiO2 nanoparticles on the adhesion strength of steel–glass/epoxy composite joints bonded with two-part structural acrylic adhesives. The introduction of nano-TiO2 in the two-part acrylic adhesive led to a remarkable enhancement in the shear and tensile strength of the composite joints. The shear and tensile strengths of the adhesive joints increased with adding the filler content up to 3 wt.%, after which it decreased with adding more filler content. Also, addition of nanoparticles caused a reduction in the peel strength of the joints. Differential scanning calorimeter analysis revealed that glass transition temperature (Tg) values of the adhesives rose with increasing the nano-filler content. The equilibrium water contact angle decreased for adhesives containing nanoparticles. Scanning electron microscope micrographs revealed that addition of nanoparticles altered the fracture morphology from smooth to rough fracture surfaces.
1 October 2014 in International Journal of Adhesion and Adhesives
This paper reports a study on the effect of silicon carbide nanoparticles on the adhesion strength of steel–glass/epoxy composite joints bonded with two-part structural acrylic adhesives. The introduction of nanosilicon carbide in the two-part acrylic adhesive led to a remarkable enhancement in the shear and tensile strength of the composite joints. The shear and tensile strengths of the adhesive joints increased with adding the filler content up to 1.5 wt%, after which decreased with adding more filler content. Also, addition of nanoparticles caused a reduction in the peel strength of the joints. DSC analysis revealed that Tg values of the adhesives rose with increase in the nanofiller content. The equilibrium water contact angle was decreased for adhesives containing nanoparticles. SEM micrographs revealed that addition of nanoparticles altered the fracture morphology from smooth to rough fracture surfaces.