The corrosion behavior of NiTi alloy and stainless steels (AISI 316L and X2CrNiMoN22-5-3) in 0.9% sodium chloride (0.154 moll-1) solution was investigated using open circuit potential measurements, potentiodynamic polarization and electrochemical impedance spectroscopy measurements. Microstructural analyses before and after electrochemical tests were performed with the scanning electron microscopy (SEM) equipped with energy dispersive spectrometry (EDS). The lowest corrosion current density has NiTi alloy and the extent of the passive range increased in the order AISI 316L stainless steel < NiTi alloy < X2CrNiMoN22-5-3 duplex stainless steel. The oxide film formed on all samples has a double-layer structure consisting of a barrier-type inner layer and a porous outer layer. Oxide films formed on the surface of steels mainly contains iron oxides and chromium oxide, while the surface film of the NiTi alloy mainly contains TiO2 oxide.
The effect of copper content (0.031 wt.% Cu, 0.32 wt.% Cu, 0.51 wt.% Cu and 0.91 wt.% Cu) on the hardness and corrosion properties of ADI was investigated. Samples austenitization were carried out at 850°C for 60 min followed by its austempering at temperatures from 250°C to 420°C for different time (30 to 60 min) in 50% (KNO3 + NaNO3) salt bath. It was concluded that hardness rises with copper content but decreases with higher austempering temperatures and times. The corrosion properties of the samples with minimum and maximum Cu content were investigated by electrochemical methods in 0.5 M NaCl solution. Samples with a higher copper content have shown higher values of polarization resistance (Rp) and lower values of corrosion current (icorr). After polarization measurements, corroded surfaces were analyzed with SEM/EDS analysis.