3 April 2017 in Nuclear Fusion
1 April 2022 in Nuclear Fusion
DIII-D physics research addresses critical challenges for the operation of ITER and the next generation of fusion energy devices. This is done through a focus on innovations to provide solutions for high performance long pulse operation, coupled with fundamental plasma physics understanding and model validation, to drive scenario development by integrating high performance core and boundary plasmas. Substantial increases in off-axis current drive efficiency from an innovative top launch system for EC power, and in pressure broadening for Alfven eigenmode control from a co-/counter-Ipsteerable off-axis neutral beam, all improve the prospects for optimization of future long pulse/steady state high performance tokamak operation. Fundamental studies into the modes that drive the evolution of the pedestal pressure profile and electron vs ion heat flux validate predictive models of pedestal recovery after ELMs. Understanding the physics mechanisms of ELM control and density pumpout by 3D magnetic perturbation fields leads to confident predictions for ITER and future devices. Validated modeling of high-Zshattered pellet injection for disruption mitigation, runaway electron dissipation, and techniques for disruption prediction and avoidance including machine learning, give confidence in handling disruptivity for future devices. For the non-nuclear phase of ITER, two actuators are identified to lower the L–H threshold power in hydrogen plasmas. With this physics understanding and suite of capabilities, a high poloidal beta optimized-core scenario with an internal transport barrier that projects nearly toQ= 10 in ITER at ∼8 MA was coupled to a detached divertor, and a near super H-mode optimized-pedestal scenario with co-Ipbeam injection was coupled to a radiative divertor. The hybrid core scenario was achieved directly, without the need for anomalous current diffusion, using off-axis current drive actuators. Also, a controller to assess proximity to stability limits and regulateβNin the ITER baseline scenario, based on plasma response to probing 3D fields, was demonstrated. Finally, innovative tokamak operation using a negative triangularity shape showed many attractive features for future pilot plant operation.
21 April 2021 in Nuclear Fusion
Silicon carbide (SiC) represents a promising but largely untested plasma-facing material (PFM) for next-step fusion devices. In this work, an analytic mixed-material erosion model is developed by calculating the physical (via SDTrimSP) and chemical (via empirical scalings) sputtering yield from SiC, Si, and C. The Si content in the near-surface SiC layer is predicted to increase during D plasma bombardment due to more efficient physical and chemical sputtering of C relative to Si. Silicon erosion from SiC thereby occurs primarily from sputtering of the enriched Si layer, rather than directly from the SiC itself. SiC coatings on ATJ graphite, manufactured via chemical vapor deposition, were exposed to repeated H-mode plasma discharges in the DIII-D tokamak to test this model. The qualitative trends from analytic modeling are reproduced by the experimental measurements, obtained via spectroscopic inference using the S/XB method. Quantitatively the model slightly under-predicts measured erosion rates, which is attributed to uncertainties in the ion impact angle distribution, as well as the effect of edge-localized modes. After exposure, minimal changes to the macroscopic or microscopic surface morphology of the SiC coatings were observed. Compositional analysis reveals Si enrichment of about 10%, in line with expectations from the erosion model. Extrapolating to a DEMO-type device, an order-of-magnitude decrease in impurity sourcing, and up to a factor of 2 decrease in impurity radiation, is expected with SiC walls, relative to graphite, if low C plasma impurity content can be achieved. These favorable erosion properties motivate further investigations of SiC as a low-Z, non-metallic PFM.
1 December 2021 in Physica Scripta
A set of experiments are planned to exploit the high SOL collisionality enabled by a tightly baffled slot divertor geometry to suppress tungsten leakage in DIII-D. A toroidal row of graphite tiles from the Small Angle Slot (SAS) divertor is being coated with 10–15 μ m of tungsten. New spectroscopic viewing chords with in-vacuo optics will measure the W gross erosion source from the divertor surface with high spatial and temporal resolution. In parallel, the bottom of the SAS divertor is changed from a flat to a ‘V’ shape. New SOLPS-ITER/DIVIMP simulations conducted with drifts using the planned ‘V’ shape predict a substantial reduction in W sourcing and SOL accumulation in either B × ∇B direction relative to either the old SAS divertor shape or the open, lower divertor. Dedicated studies are planned to carefully characterize the level of W sourcing, leakage, and scrape-off-layer (SOL) accumulation in DIII-D over a wide range of plasma scenarios. Various actuators will be assessed for their efficacy in further reducing high-Z impurity sources and leakage from the slot divertor geometry. This coupled code-experiment validation effort will be used to stress-test physics models and build confidence in extrapolations to advanced, high-Z divertor geometries for next-step devices.
24 October 2017 in Physica Scripta
Unipolar arcing was an important mechanism of metal surface erosion during the recently conducted Metal Rings Campaign in DIII-D when two toroidally continuous tile rings with 5 cm wide W-coated TZM inserts were installed in graphite tiles in the lower divertor, one on the floor and one on the shelf. Most of the arc damage occurred on the shelf ring. The total amount of W removed by arcing from the affected ~4% of the shelf ring area was estimated ~0.8 × 1021 at., about half of the total amount of W eroded and redeposited outside the inserts (1.8 ± 0.9)×1021 at. The rings were exposed for a total of ~480 discharges, an equivalent of plasma time on W surfaces (with MA) ~103 s. Arcing was monitored in situ with WI (400.9 nm) filtered camera and photomultipliers and showed that: (i) arcing only occurred during ELMs and disruptions, (ii) arcing rate was much lower on the floor than on the shelf ring, and (iii) arcing had a low cut off power flux density about 2 MW m−2. About half of arc tracks had large pitch angle and probably were produced during disruptions. Such tracks were only found on the shelf. Moderate toroidal variation of the arc track density and W erosion with nearly n = 1 pattern has been measured.
5 February 2018 in IEEE Transactions on Plasma Science
ABAlexis R. Briesemeister
Recent emphasis of tungsten (W) plasma-material interaction experiments on DIII-D has made it essential to enhance the W I and W II measurement capabilities of its spectroscopy diagnostic suite to acquire W sourcing measurements with high temporal, spatial, and wavelength resolution. To this end, four new viewing chords for the multichordal divertor spectrometer and divertor filterscope systems were installed, leading to a 7× increase in blue-light sensitivity. W I and low-Z impurity line identifications were performed in the 3995-4030 Å region, placing wavelengths within 0.1 Å of the National Institute of Standards and Technology values. A novel method was also developed for the DIII-D high-temporal resolution filterscopes to distinguish between W I light and background contamination, important due to the relatively weak intensity of this line, using two different bandpass filters with different widths but the same center wavelength. Finally, fast imaging of the W I 4008.75 Å spectral line with a PCO Pixelfly VGA 200/205 camera is allowed for discrimination between intra-edge-localized mode (ELM) and inter-ELM W I emission profiles with very high (~1 mm) spatial resolution.