18 July 2022 in Journal of Physics D: Applied Physics
The ZnO fibers (Fs)/p-Si (labeled D1) and ZnO Fs/n-Si (labeled D2) photodetector heterojunctions were fabricated and both devices gave a clear rectifying I–V characteristic with a high rectifying ratio, in the dark. At zero bias, D1 showed self-driven characteristics, while D2 had not and D1 was found to be more stable than D2 in time-dependent measurements. Optoelectronics results revealed that D1 had high sensitivity to both visible and excellent stability after 20 days. At zero bias, the ON/OFF ratio of the D1 photodetector was as high as 33 650 and in the dark, a rectification ratio of 67 400 within ±2 V was obtained for the D1 device. The maximum responsivities of the devices was ∼0.8 mA W−1, and their detectivity was ∼109 Jones. Furthermore, the ZnO Fs/p-Si (labeled D3) and ZnO Fs/n-Si (labeled D3) photodetectors yielded excellent response to 365 nm and 395 nm UV light (10 mW cm−2). Responsivity, detectivity (D), and external quantum efficiency values reached as high as 5.28 A W−1, 1.02 × 1013 Jones, and %16.6, respectively under 365 nm UV light. The excellent responses of the photodetectors to visible and UV light were attributed to the oxygen vacancies in ZnO and the formation of electron–hole pairs by the light effect and their separation by the electric field in the device formed between ZnO and Si.
22 August 2022 in Journal of Physics D: Applied Physics
In this work, the electrical and photoresponse measurements of a transparent conductive Al-doped ZnO (AZO)/n-Si heterojunction device were conducted in visible light and UV wavelengths. AZO film was deposited by sputtering onto an n-Si wafer and investigated by means of morphological, chemical and electrical characterizations. The AZO/n-Si rectifying device exhibits an excellent reproducibility without noticeable variations after 90 days of measurements. At self-powered mode, the maximum on/off ratios were determined as 3081 for visible light and 4778 for UV light illumination of 365 nm. The responsivity and detectivity of the AZO/n-Si photodetector were 0.128 A W−1 and 1.05 × 1011 Jones for 365 nm, whereas they were 0.055 A W−1 and 4.60 × 1010 Jones for 395 nm, respectively (at −2.0 V). This study demonstrated that the n-AZO/n-Si isotype heterojunction photodetector was fabricated at low cost and it is a potential candidate in both the visible region and the UV region with a good performance, in contrast to the widely studied pn heterojunctions.
30 November 2023 in Physica Scripta
A Hibiscus sabdariffa (HBS)/n-Si hybrid photodetector was fabricated and it was observed that the device has a high rectification ratio of 10.2 × 104 in dark and superior photoresponse at different intensities of visible light in addition to UV and IR lights. The non-linear response to light intensity in visible light was attributed to phase change effects and the presence of traps, which are the result of the hibiscus sabdariffa’ response to light. The responsivity at 850 nm reaches 1.16 A W−1 (at V = −2.0 V) and a high specific detectivity of 2.0 × 1012 Jones (for self-driven mode) with an external quantum efficiency of 411% was obtained. In addition, in self-driven mode of UV and IR lights, the highest on/off ratio and NPDR values reached ∼105 and ∼109 W−1 levels, respectively. Moreover, HBS/n-Si hybrid broad-band photodetector showed long-term stability (40 days) without encapsulation both in the dark and under the light.
9 November 2023 in Organic Electronics
9 May 2024 in Journal of the American Ceramic Society
This study aims to reveal the growth kinetics of ZnO nanoflakes and ZnO/GO nanocomposite films obtained at different Zn precursor salt concentrations by electrochemical deposition method and to evaluate the catalytic performances of the obtained films. The films were grown on FTO substrate with Zn precursor salt concentrations of 0.1 M, 0.125 M, and 0.175 M. Characterization of the obtained films was performed by XRD, SEM, UV–vis–NIR, Raman, and XPS analyses. The strong photocatalytic capabilities of the synthesized ZnO nanoflakes and ZnO/GO nanocomposite films were demonstrated by comparative analyses with the existing literature. Accordingly, photocatalytic experiments carried out under UVA irradiation revealed the high performance of the synthesized samples in the degradation of MB dye. The reaction kinetics were investigated using the Langmuir‐Hinshelwood kinetic model, resulting in high kobs values and R2 coefficients. ZnO nanoparticles showed a kobs of 0.038 min−1 and an R2 value of 0.96, while ZnO/GO nanocomposite films showed a kobs of 0.055 min−1 and an R2 value of 0.92. The significant increase in the degradation percentage shows the significant improvement achieved by the integration of GO, despite a slightly lower R2 value for the ZnO/GO nanocomposite film compared with ZnO nanoflakes films.
23 December 2022 in Physica Scripta
Both Polyvinylpyrrolidone (PVP) and matrix-polymer of carbon (C)-PVP fibers (Fs) composites were synthesized by using the electrospinning technique and deposited onto the p-Si wafers to obtain PVP Fs/p-Si and C-PVP Fs/p-Si devices. The ultraviolet/Visible (UV/Vis) photodetector performance of both devices was compared. Both devices gave self-powered mode and with increasing the visible light intensity, the photocurrents of both devices increased. Besides, it was observed that the optical performance of the device containing C was better than the PVP Fs/p-Si device in both visible and UV lights. This was attributed to the high absorption properties of carbon and the increase in conductivity in the PVP due to carbon fibers. Furthermore, it is thought that the electric field formed in the carbon-PVP interaction and C-PVP/p-Si interface improves the optical properties of the device by increasing the exciton separation efficiency. Under the self-powered mode, the C-PVP Fs/p-Si device exhibited a maximum detectivity and ON/OFF ratio of 5.60 × 1010 Jones and 53 764, respectively for UV light of 365 nm. Under 100 mW visible light, these values were determined as 1.01 × 1010 Jones and 9739, respectively, at V = 0. In addition, from the obtained noise-equivalent power (NEP) values, it was concluded that weaker signals can be detected under UV light (6.94 × 10−14 w Hz−1/2, at −2 V) than visible light (3.32 × 10−13 w/Hz1/2, at −2 V) for C-PVP Fs/p-Si.