This work investigated the feasibility of manufacturing composite cross-laminated timber (CCLT) from bamboo and a western hemlock and amabilis fir mix (hem-fir). Bamboo parallel strand lumber (bamboo PSL) was first fabricated as the surface laminae of CCLT. No. 2 and Btr 2×6 western hem-fir dimension lumber was imported from British Columbia (BC), Canada. The lumber was then sorted and further dried to form the inner laminae of CCLT. Multiple 800 × 800-mm CLT billets were fabricated using a commercial single-component polyurethane (PUR) adhesive. Block shear and delamination tests were conducted to examine the bond quality and durability of bamboo-wood CCLT. The results demonstrated that it is technically feasible to manufacture bamboo-wood CCLT with acceptable bond quality (shear strength, wood failure percentage, etc.) and delamination. Further studies should focus on the optimization of process parameters for manufacturing and surface treatment to improve the bond quality and durability and quantify the mechanical performance of bamboo-wood CCLT with a full-size production trial.
A novel flattened bamboo-wood composite cross-laminated timber (CCLT) made from flattened bamboo and hemlock lumber was developed, and its mechanical performance was investigated and quantified in this work. The results demonstrated that the CCLT columns and control hemlock CLT counterparts had nearly equal axial compression strength, but the CCLT yielded a higher compression modulus of elasticity (MOE). Additionally, the CCLT compression behaviors were not significantly affected by the height. Compared with hemlock CLT, the CCLT exhibited a slightly higher flatwise bending MOE and strength in the major strength direction. Furthermore, the MOE and strength of the CCLT under edgewise bending were 17.3% less and 16.2% greater than those under flatwise bending, respectively. The load-carrying capacity of the CCLT was mainly governed by the interfacial failure between the bamboo and wood, in which no rolling shear failure was observed. Those features are unique for the new CCLT for engineered applications.
10 July 2017 in Journal of Sandwich Structures & Materials
To increase the engineering applications of basalt fiber, the characteristics of the shear mechanical properties and the influence mechanisms of the fiber length ( Lf) and volume fraction ( Vf) for short basalt fiber reinforced epoxy resin polymer composites were investigated. The following results were obtained: (1) The first critical loads on all the shear load–displacement curves are close to the same value due to having the same interface bonding of the fiber–matrix; (2) the shear strength, deformation, and energy dissipation capacity all increase with increasing Vf; however, when Lf is 6 or 9 mm, these increases are slower, whereas when Lf is 3 mm, these values increase at an approximately constant rate; and (3) the shear elastic modulus of the samples reaches its maximum value when Lf is 3 mm and Vf is 25%; however, it increases more quickly when Lf is 6 or 9 mm. The failure mode of the samples with the larger Lf values is mainly debonding between the fiber and matrix; when Vf is high, the fibers can easily bundle, which reduces the adhesion between the fibers and matrix. In addition, the main failure mode of the 3-mm-long fiber samples is fiber pull-out; when Vf is high, the short fibers that are not pulled out significantly increase the deformation ability.