A modified sol-gel process was studied as applied to synthesize a lithium-conducting solid electrolyte of composition Li1.3Al0.3Ti1.7(PO4)3 (LATP) using water-soluble salts Al(NO3)3 · 9H2O, LiNO3 · 3H2O, and (NH4)2HPO4 and a titanium(IV) citrate complex. As-synthesized samples were characterized using X-ray powder diffraction, DSC/TG, SEM, and impedance spectroscopy. Sintering of as-synthesized amorphous powders at 700°C was found to yield LATP with crystallite sizes of 42–48 nm. Ionic conductivity of the electrolyte measured in the frequency range 25–106 Hz in disks having 86–90% density that were sintered at 1000°C was (3–4) × 10−4 S/cm. Temperature-dependent ionic conductivity was studied in the range 25–200°C. The activation energy of conduction was determined for LATP.
Comprehensive studies have been carried out of the interconnection of the properties of the initial powders and characteristics of optical scintillation ZnO ceramics obtained by uniaxial hot pressing. It is established how the lattice parameters, the texture, and the transparency of the ceramic samples depend on the type of powder. The x-ray luminescence intensity of the optical scintillation ZnO ceramics, with an emission wavelength peak at 517 nm, equals about 50% of that for CsI : Tl and is comparable to that of GOS : Pr, Ce ceramic, with a mean fluorescence time of 1.0–1.6 µs. The total transmittance of 1.0-mm-thick ceramic samples is about 45% at a wavelength of 517 nm.
The dielectric permittivity of LixNa1 − xNbO3 ferroelectric solid solutions prepared at high pressures has been measured as a function of temperature and frequency, and their structural properties have been studied. The results demonstrate that ceramics samples of the LixNa1 − xNbO3 (x = 0.17, 0.25) ferroelectric perovskite solid solutions exhibit superionic conduction at relatively low temperatures (T ≥ 400 K). In the temperature range of superionic conduction, we observe significant dielectric dispersion and anomalies in permittivity, corresponding to structural transformations of the high-pressure solid solutions.
Phase-pure BaTiO3 powder (free of Ba2TiO4, BaCO3, Ba(NO3)2, and OH impurities) with an average particle size of about 100 nm is prepared by solid-state reaction between titanium oxyhydroxide and barium hydroxide ground and mixed by sonication in an inert organic liquid.
25 September 2014 in Russian Journal of Inorganic Chemistry
The process for producing the electrode material LiCoPO4 modified by the lithium-conducting solid electrolyte Li1.3Al0.3Ti1.7(PO4)3 (LATP) was studied. To create a composite consisting of an electrochemically active substance and an electrically conductive additive distributed uniformly between LiCoPO4 particles, a peroxide solution of a LATP precursor was used. After annealing at 700°C, the two-phase composite LiCoPO4/LATP was obtained, the conductivity of which was two orders of magnitude higher than that of binary lithium cobalt phosphate at room temperature.